IS 1570 (Part 5) X66Cr13 vs EN 10088-3 X46Cr13

Close Alternative — 81.7% match based on chemical composition and mechanical property overlap.

IS 1570 (Part 5) X66Cr13 (IS 1570 (Part 5):1985) and EN 10088-3 X46Cr13 (EN 10088-3:2014) are both steel grades. Both fall under the Stainless Steel category. IS 1570 (Part 5) X66Cr13 is defined under Bureau of Indian Standards (IS), originating from India, while EN 10088-3 X46Cr13 is defined under European Standard (EN), originating from Europe.

As per chemical composition, IS 1570 (Part 5) X66Cr13 vs EN 10088-3 X46Cr13 is a 81.7% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a close alternative overall at 81.7%.

Frequently Compared With IS 1570 (Part 5) X66Cr13:
GOST 5632 08X18H10 GOST 5632 12Kh13 EN 10088-1 1.4006 EN 10088-1 1.4301 GB/T 3280 06Cr19Ni10 GOST 5632 06Kh23N28 EN 10088-1 1.4401 EN 10088-1 1.4845 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12Ni2Mo ASTM A959 .-
Match Breakdown
CHEMISTRY MATCH
81.7%
MECHANICAL MATCH
No shared data
OVERALL
81.7%
Specifications
Property IS 1570 (Part 5) X66Cr13 EN 10088-3 X46Cr13
Standard IS 1570 (Part 5):1985 EN 10088-3:2014
Category Stainless Steel Stainless Steel
C (%) 0.60-0.72 0.43-0.50
Si (%) <=0.5 <=1.00
Mn (%) 0.40-1.0 <=1.00
Cr (%) 12.0-14.0 12.5-14.5
P (%) Not specified <=0.040
S (%) Not specified <=0.030
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property IS 1570 (Part 5) X66Cr13 EN 10088-3 X46Cr13
Tensile Strength Not specified <=800 MPa
Hardness Not specified <=245 HB
Condition Not specified Annealed (+A), conditions 1C, 1E, 1D, 1X, 1G and 2D, size range not stated; hardness for guidance only
Typical Applications
IS 1570 (Part 5) X66Cr13
Not documented
EN 10088-3 X46Cr13
General purposes, semi-finished products, bars, rods, wire, sections and bright products
Key Differences
Can IS 1570 (Part 5) X66Cr13 Be Substituted With EN 10088-3 X46Cr13?
IS 1570 (Part 5) X66Cr13 and EN 10088-3 X46Cr13 are a close alternative rather than a direct substitute. Some properties overlap well, but check the specific chemistry and mechanical rows above against your application's requirements before treating them as interchangeable.
On M-EX Right Now
IS 1570 (Part 5) X66Cr13
0 active listings and RFQs →
EN 10088-3 X46Cr13
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between IS 1570 (Part 5) X66Cr13 and EN 10088-3 X46Cr13?
EN 10088-3 X46Cr13 specifies P, S which are not specified for IS 1570 (Part 5) X66Cr13.
Can IS 1570 (Part 5) X66Cr13 be substituted with EN 10088-3 X46Cr13?
IS 1570 (Part 5) X66Cr13 and EN 10088-3 X46Cr13 are a close alternative rather than a direct substitute. Some properties overlap well, but check the specific chemistry and mechanical rows above against your application's requirements before treating them as interchangeable.