IS 6911 X04Cr19Ni9 vs GB/T 3280 06Cr19Ni10

Related Material — 63.7% match based on chemical composition and mechanical property overlap.

IS 6911 X04Cr19Ni9 (IS 6911:1992) and GB/T 3280 06Cr19Ni10 (GB/T 3280-2015) are both steel grades. Both fall under the Stainless Steel category. IS 6911 X04Cr19Ni9 is typically used for used in food equipment, chemical processing units, kitchenware, tanks, piping, and architectural applications., while GB/T 3280 06Cr19Ni10 is commonly used for used for kitchen equipment, food processing machinery, chemical tanks, piping, architectural panels, and fasteners.. IS 6911 X04Cr19Ni9 is defined under Bureau of Indian Standards (IS), originating from India, while GB/T 3280 06Cr19Ni10 is defined under Guobiao Standards (GB/T), originating from China.

As per chemical composition, IS 6911 X04Cr19Ni9 vs GB/T 3280 06Cr19Ni10 is a 95.6% match. As per mechanical properties, the match is 0%. Combined, this makes them a related material overall at 63.7%.

Frequently Compared With IS 6911 X04Cr19Ni9:
EN 10088-1 1.4845 EN 10088-1 1.4006 GOST 5632 08X18H10 EN 10088-1 1.4401 GOST 5632 12Kh13 EN 10088-1 1.4301 GOST 5632 06Kh23N28 IS 1570 (Part 7) 12Cr12MoVH IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12Ni2Mo ASTM A959 .- IS 1570 (Part 7) 11Cr17Ni13W3TiH
Match Breakdown
CHEMISTRY MATCH
95.6%
MECHANICAL MATCH
0%
OVERALL
63.7%
Specifications
Property IS 6911 X04Cr19Ni9 GB/T 3280 06Cr19Ni10
Standard IS 6911:1992 GB/T 3280-2015
Category Stainless Steel Stainless Steel
C (%) <=0.08 0.08 max
Cr (%) 17.5-20.0 18.00-20.00
Mn (%) <=2.0 2.00 max
Ni (%) 8.0-10.0 8.00-11.00
P (%) <=0.045 0.045 max
S (%) <=0.030 0.030 max
Si (%) <=1.0 1.00 max
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property IS 6911 X04Cr19Ni9 GB/T 3280 06Cr19Ni10
Bend Test (180 deg) Not required Not specified
Elongation (50 mm, annealed) >=40% Not specified
Hardness (annealed, max) 192 HBS, 92 HRB Not specified
Tensile Strength (annealed) >=400 MPa Not specified
Yield Strength (0.2% proof, annealed) >=200 MPa Not specified
Tensile Strength Not specified 520-720 MPa
Yield Strength Not specified 205-310 MPa
Elongation Not specified 40-60%
Hardness Not specified 187 HB max
Typical Applications
IS 6911 X04Cr19Ni9
Used in food equipment, chemical processing units, kitchenware, tanks, piping, and architectural applications.
GB/T 3280 06Cr19Ni10
Used for kitchen equipment, food processing machinery, chemical tanks, piping, architectural panels, and fasteners.
Can IS 6911 X04Cr19Ni9 Be Substituted With GB/T 3280 06Cr19Ni10?
IS 6911 X04Cr19Ni9 and GB/T 3280 06Cr19Ni10 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
Forms & Sizes Available on M-EX
IS 6911 X04Cr19Ni9
Sheet → (2 listings)
Thickness: 6–6 mm (0.24–0.24 in)
Width: 1250–1250 mm (49.21–49.21 in)
Length: 2600–3500 mm (102.36–137.8 in)
GB/T 3280 06Cr19Ni10
Sheet → (2 listings)
Thickness: 6–6 mm (0.24–0.24 in)
Width: 1250–1250 mm (49.21–49.21 in)
Length: 2900–3300 mm (114.17–129.92 in)
On M-EX Right Now
IS 6911 X04Cr19Ni9
2 active listings and RFQs →
GB/T 3280 06Cr19Ni10
2 active listings and RFQs →
Frequently Asked Questions
What is the difference between IS 6911 X04Cr19Ni9 and GB/T 3280 06Cr19Ni10?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can IS 6911 X04Cr19Ni9 be substituted with GB/T 3280 06Cr19Ni10?
IS 6911 X04Cr19Ni9 and GB/T 3280 06Cr19Ni10 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.