IS 6911 X04Cr17Ni12Mo2Ti vs ASTM A959 SS316

Strong Match — 100% match based on chemical composition and mechanical property overlap.

IS 6911 X04Cr17Ni12Mo2Ti (IS 6911:1992) and ASTM A959 SS316 (ASTM A959:2011) are both steel grades. Both fall under the Stainless Steel category. IS 6911 X04Cr17Ni12Mo2Ti is typically used for stainless and heat-resisting steel plate, sheet and strip (clause 1.1), while ASTM A959 SS316 is commonly used for marine, chemical, pharmaceutical, food processing equipment. IS 6911 X04Cr17Ni12Mo2Ti is defined under Bureau of Indian Standards (IS), originating from India, while ASTM A959 SS316 is defined under ASTM International, originating from United States.

As per chemical composition, IS 6911 X04Cr17Ni12Mo2Ti vs ASTM A959 SS316 is a 100% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a strong match overall at 100%.

Frequently Compared With IS 6911 X04Cr17Ni12Mo2Ti:
EN 10088-1 1.4006 EN 10088-1 1.4845 GOST 5632 08X18H10 EN 10088-1 1.4401 IS 1570 (Part 7) 12Cr12Ni2Mo GOST 5632 06Kh23N28 EN 10088-1 1.4301 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoH GB/T 3280 06Cr19Ni10 IS 1570 (Part 7) 12Cr12MoVH IS 1570 (Part 7) 12Cr13H
Match Breakdown
CHEMISTRY MATCH
100%
MECHANICAL MATCH
No shared data
OVERALL
100%
Specifications
Property IS 6911 X04Cr17Ni12Mo2Ti ASTM A959 SS316
Standard IS 6911:1992 ASTM A959:2011
Category Stainless Steel Stainless Steel
C (%) <=0.08 <=0.08
Cr (%) 16.0-18.0 16.0-18.0
Mn (%) <=2.0 <=2.00
Mo (%) 2.0-3.0 2.00-3.00
Ni (%) 10.0-14.0 10.0-14.0
P (%) <=0.045 <=0.045
S (%) <=0.030 <=0.030
Si (%) <=1.0 <=1.00
Ti (%) >=5x(C+N), <=0.80 Not specified
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property IS 6911 X04Cr17Ni12Mo2Ti ASTM A959 SS316
Bend Test (180 deg) Not required Not specified
Elongation (50 mm, annealed) >=35% Not specified
Hardness (annealed, max) 192 HBS, 95 HRB Not specified
Tensile Strength (annealed) >=490 MPa Not specified
Yield Strength (0.2% proof, annealed) >=220 MPa Not specified
Typical Applications
IS 6911 X04Cr17Ni12Mo2Ti
Stainless and heat-resisting steel plate, sheet and strip (clause 1.1)
ASTM A959 SS316
Marine, chemical, pharmaceutical, food processing equipment
Key Differences
Can IS 6911 X04Cr17Ni12Mo2Ti Be Substituted With ASTM A959 SS316?
IS 6911 X04Cr17Ni12Mo2Ti and ASTM A959 SS316 overlap closely enough on chemistry and mechanical properties that ASTM A959 SS316 is often considered as a substitute for IS 6911 X04Cr17Ni12Mo2Ti in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
Forms & Sizes Available on M-EX
IS 6911 X04Cr17Ni12Mo2Ti
No active listings currently.
ASTM A959 SS316
Sheet → (24 listings)
Thickness: 2–6 mm (0.08–0.24 in)
Width: 1250–1250 mm (49.21–49.21 in)
Length: 2500–4000 mm (98.43–157.48 in)
Plate → (6 listings)
Thickness: 10–10 mm (0.39–0.39 in)
Width: 1500–1500 mm (59.06–59.06 in)
Length: 2600–4200 mm (102.36–165.35 in)
Round Bar → (3 listings)
Diameter: 40–40 mm (1.57–1.57 in)
Length: 2500–4200 mm (98.43–165.35 in)
On M-EX Right Now
IS 6911 X04Cr17Ni12Mo2Ti
0 active listings and RFQs →
ASTM A959 SS316
33 active listings and RFQs →
Frequently Asked Questions
What is the difference between IS 6911 X04Cr17Ni12Mo2Ti and ASTM A959 SS316?
IS 6911 X04Cr17Ni12Mo2Ti specifies Ti which is not specified for ASTM A959 SS316.
Can IS 6911 X04Cr17Ni12Mo2Ti be substituted with ASTM A959 SS316?
IS 6911 X04Cr17Ni12Mo2Ti and ASTM A959 SS316 overlap closely enough on chemistry and mechanical properties that ASTM A959 SS316 is often considered as a substitute for IS 6911 X04Cr17Ni12Mo2Ti in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.