IS 6911 X15Cr16Ni2 vs EN 10088-1 X17CrNi16-2

Strong Match — 92% match based on chemical composition and mechanical property overlap.

IS 6911 X15Cr16Ni2 (IS 6911:1992) and EN 10088-1 X17CrNi16-2 (EN 10088-1:2014) are both steel grades. Both fall under the Stainless Steel category. IS 6911 X15Cr16Ni2 is defined under Bureau of Indian Standards (IS), originating from India, while EN 10088-1 X17CrNi16-2 is defined under European Standard (EN), originating from Europe.

As per chemical composition, IS 6911 X15Cr16Ni2 vs EN 10088-1 X17CrNi16-2 is a 92% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a strong match overall at 92%.

Frequently Compared With IS 6911 X15Cr16Ni2:
ASTM A959 205 EN 10088-1 1.4006 EN 10088-1 1.4301 EN 10088-1 1.4401 EN 10088-1 1.4845 GB/T 3280 06Cr19Ni10 GOST 5632 06Kh23N28 GOST 5632 08X18H10 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12MoVH ASTM A959 .-
Match Breakdown
CHEMISTRY MATCH
92%
MECHANICAL MATCH
No shared data
OVERALL
92%
Specifications
Property IS 6911 X15Cr16Ni2 EN 10088-1 X17CrNi16-2
Standard IS 6911:1992 EN 10088-1:2014
Category Stainless Steel Stainless Steel
C (%) 0.10-0.20 0.12-0.22
Cr (%) 15.0-17.0 15.0-17.0
Mn (%) <=1.0 <=1.50
Ni (%) 1.25-2.50 1.50-2.50
P (%) <=0.045 <=0.040
S (%) <=0.030 <=0.015
Si (%) <=1.0 <=1.00
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property IS 6911 X15Cr16Ni2 EN 10088-1 X17CrNi16-2
Elongation (50 mm, annealed) >=10% Not specified
Hardness (annealed, max) 262 HBS Not specified
Tensile Strength (annealed) >=830 MPa Not specified
Yield Strength (0.2% proof, annealed) >=640 MPa Not specified
Typical Applications
IS 6911 X15Cr16Ni2
Stainless and heat-resisting steel plate, sheet and strip (clause 1.1)
EN 10088-1 X17CrNi16-2
Not documented
Can IS 6911 X15Cr16Ni2 Be Substituted With EN 10088-1 X17CrNi16-2?
IS 6911 X15Cr16Ni2 and EN 10088-1 X17CrNi16-2 overlap closely enough on chemistry and mechanical properties that EN 10088-1 X17CrNi16-2 is often considered as a substitute for IS 6911 X15Cr16Ni2 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
On M-EX Right Now
IS 6911 X15Cr16Ni2
0 active listings and RFQs →
EN 10088-1 X17CrNi16-2
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between IS 6911 X15Cr16Ni2 and EN 10088-1 X17CrNi16-2?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can IS 6911 X15Cr16Ni2 be substituted with EN 10088-1 X17CrNi16-2?
IS 6911 X15Cr16Ni2 and EN 10088-1 X17CrNi16-2 overlap closely enough on chemistry and mechanical properties that EN 10088-1 X17CrNi16-2 is often considered as a substitute for IS 6911 X15Cr16Ni2 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.