JIS G4304:2021 SUS304N1 Steel: Specifications & Listings

JIS G4304:2021 SUS304N1: SUS304N1: austenitic stainless steel, hot-rolled plate, sheet and strip. Specified in JIS G 4304:2021.

Category: Stainless Steel
Grade Details
GradeJIS G4304:2021 SUS304N1
Standard JIS G4304:2021
ApplicationsHot-rolled stainless steel plates and strips
Equivalent / Similar Grades
Grade Standard Region Live on M-EX
ASTM A959 XM-21 ASTM A959:2011 USA No activity yet
EN 10088-1 X5CrNiN19-9 EN 10088-1:2014 Europe (CEN) No activity yet
JIS G4305 SUS304N1 JIS G4305:2012 Japan No activity yet
ASTM A959 304N ASTM A959:2011 USA No activity yet
ASTM A959 SS304 ASTM A959:2011 USA 16 listings, 18 RFQs →
EN 10088-1 X5CrNi18-10 EN 10088-1:2014 Europe (CEN) 3 listings, 0 RFQs →
ASTM A959 304H ASTM A959:2011 USA No activity yet
Grade ComparisonCompare With a Specific Grade →
Grade Standard Match
JIS G4305 SUS304N1 JIS G4305:2012 Strong Match
ASTM A959 304N ASTM A959:2011 Strong Match
ASTM A959 XM-21 ASTM A959:2011 Strong Match
EN 10088-1 X5CrNiN19-9 EN 10088-1:2014 Strong Match
EN 10088-1 X5CrNiN19-9 EN 10088-1:2023 Strong Match
ASTM A959 SS304 ASTM A959:2011 Strong Match
EN 10088-1 X5CrNi18-10 EN 10088-1:2014 Strong Match
ASTM A959 304H ASTM A959:2011 Strong Match
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Chemical Composition (%)
C Si Mn P S Ni Cr N
<=0.08 <=1.00 <=2.50 <=0.045 <=0.030 7.00-10.50 18.00-20.00 0.10-0.25
Mechanical Properties
Tensile Strength >=550 MPa
Yield Strength >=275 MPa
Elongation >=35%
Hardness <=217 HB
Condition Solution heat treated plate and strip; 0.2 percent proof strength applies only when specified by the purchaser

More data from JIS G4304:2021

From the standard
Mechanical properties, solution heat treated 3 values
0.2 percent proof strength, min
275 MPa
Tensile strength, min
550 MPa
Elongation, min
35 %
0.2 percent proof strength applies only when specified by the purchaser. 1 N/mm2 = 1 MPa.
Source: JIS G 4304:2021, Table 8
Hardness, solution heat treated 3 scales
Brinell hardness HBW, max
217
Rockwell HRBW or HRBS, max
95
Vickers hardness HV, max
220
Any one of the hardness scales applies; if not specified the manufacturer selects. HRBW is used in case of dispute.
Source: JIS G 4304:2021, Table 8
Heat treatment (example, informative) 1 settings
Solution heat treatment
1010 to 1150 deg C, rapid cooling
Annex JA is informative; temperatures are examples.
Source: JIS G 4304:2021, Table JA.1

Active JIS G4304:2021 SUS304N1 Listings on M-EX (For Sale)

+ Create a Listing for this grade

No active JIS G4304:2021 SUS304N1 listings at this time.

Register for Alerts

Buyer RFQs for JIS G4304:2021 SUS304N1

+ Post an RFQ for this grade

No open buyer requirements for JIS G4304:2021 SUS304N1 at this time.

Register for Alerts