Minimal Match — 34.5% match
based on chemical composition and mechanical property overlap.
JIS G4305 SUS304N2 (JIS G4305:2012) and EN 10088-1 1.4401 (EN 10088-1:2014) are both steel grades.
Both fall under the Stainless Steel category.
JIS G4305 SUS304N2 is typically used for cold-rolled stainless steel plates, sheet and strip, while EN 10088-1 1.4401 is commonly used for marine, chemical processing, pharmaceutical equipment.
JIS G4305 SUS304N2 is defined under Japanese Industrial Standards (JIS), originating from Japan, while EN 10088-1 1.4401 is defined under European Standard (EN), originating from Europe.
As per chemical composition, JIS G4305 SUS304N2 vs EN 10088-1 1.4401 is a 51.7% match.
As per mechanical properties, the match is 0%.
Combined, this makes them a minimal match overall at 34.5%.
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property
JIS G4305 SUS304N2
EN 10088-1 1.4401
Tensile Strength
>=690 MPa
≥520 MPa
Yield Strength
>=345 MPa
≥210 MPa
Elongation
>=35%
≥40%
Hardness
<=248 HB
≤215 HB
Condition
Solution heat treated plate and strip; 0.2 percent proof strength applies only when specified by the purchaser
Not specified
Typical Applications
JIS G4305 SUS304N2
Cold-rolled stainless steel plates, sheet and strip
EN 10088-1 1.4401
Marine, chemical processing, pharmaceutical equipment
Key Differences
JIS G4305 SUS304N2 specifies P, S, N, Nb which are not specified for EN 10088-1 1.4401.
EN 10088-1 1.4401 specifies Mo which is not specified for JIS G4305 SUS304N2.
Can JIS G4305 SUS304N2 Be Substituted With EN 10088-1 1.4401?
JIS G4305 SUS304N2 and EN 10088-1 1.4401 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
What is the difference between JIS G4305 SUS304N2 and EN 10088-1 1.4401?
JIS G4305 SUS304N2 specifies P, S, N, Nb which are not specified for EN 10088-1 1.4401. EN 10088-1 1.4401 specifies Mo which is not specified for JIS G4305 SUS304N2.
Can JIS G4305 SUS304N2 be substituted with EN 10088-1 1.4401?
JIS G4305 SUS304N2 and EN 10088-1 1.4401 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.