JIS G4305 SUS305 vs EN 10088-1 1.4845

Minimal Match — 35% match based on chemical composition and mechanical property overlap.

JIS G4305 SUS305 (JIS G4305:2012) and EN 10088-1 1.4845 (EN 10088-1:2014) are both steel grades. Both fall under the Stainless Steel category. JIS G4305 SUS305 is typically used for cold-rolled stainless steel plates, sheet and strip, while EN 10088-1 1.4845 is commonly used for furnace parts, heat exchangers, kiln components. JIS G4305 SUS305 is defined under Japanese Industrial Standards (JIS), originating from Japan, while EN 10088-1 1.4845 is defined under European Standard (EN), originating from Europe.

As per chemical composition, JIS G4305 SUS305 vs EN 10088-1 1.4845 is a 66.4% match. As per mechanical properties, the match is 33.3%. Combined, this makes them a minimal match overall at 35%.

Frequently Compared With JIS G4305 SUS305:
ASTM A959 .- GB/T 3280 06Cr19Ni10 GOST 5632 08X18H10 EN 10088-1 1.4006 EN 10088-1 1.4301 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12Ni2Mo
Other Stainless Steel Grades to Compare With JIS G4305 SUS305:
GOST 5632 06Kh23N28 EN 10088-1 1.4401 IS 1570 (Part 7) 12Cr12MoVH IS 1570 (Part 7) 12Cr13H
Match Breakdown
CHEMISTRY MATCH
66.4%
MECHANICAL MATCH
33.3%
OVERALL
35%
Specifications
Property JIS G4305 SUS305 EN 10088-1 1.4845
Standard JIS G4305:2012 EN 10088-1:2014
Category Stainless Steel Stainless Steel
C (%) <=0.12 ≤0.10
Si (%) <=1.00 ≤1.50
Mn (%) <=2.00 ≤2.00
P (%) <=0.045 Not specified
S (%) <=0.030 Not specified
Ni (%) 10.50-13.00 19.0–22.0
Cr (%) 17.00-19.00 24.0–26.0
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property JIS G4305 SUS305 EN 10088-1 1.4845
Tensile Strength >=480 MPa ≥515 MPa
Yield Strength >=175 MPa ≥205 MPa
Elongation >=40% ≥40%
Hardness <=187 HB Not specified
Condition Solution heat treated plate and strip; 0.2 percent proof strength applies only when specified by the purchaser Not specified
Max Service Temp Not specified 1100°C continuous
Typical Applications
JIS G4305 SUS305
Cold-rolled stainless steel plates, sheet and strip
EN 10088-1 1.4845
Furnace parts, heat exchangers, kiln components
Key Differences
Can JIS G4305 SUS305 Be Substituted With EN 10088-1 1.4845?
JIS G4305 SUS305 and EN 10088-1 1.4845 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
Forms & Sizes Available on M-EX
JIS G4305 SUS305
No active listings currently.
EN 10088-1 1.4845
Sheet → (3 listings)
Thickness: 6–6 mm (0.24–0.24 in)
Width: 1250–1250 mm (49.21–49.21 in)
Length: 2700–3200 mm (106.3–125.98 in)
On M-EX Right Now
JIS G4305 SUS305
0 active listings and RFQs →
EN 10088-1 1.4845
3 active listings and RFQs →
Frequently Asked Questions
What is the difference between JIS G4305 SUS305 and EN 10088-1 1.4845?
JIS G4305 SUS305 specifies P, S which are not specified for EN 10088-1 1.4845.
Can JIS G4305 SUS305 be substituted with EN 10088-1 1.4845?
JIS G4305 SUS305 and EN 10088-1 1.4845 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.