JIS G4305:2012 SUS312L Steel: Specifications & Listings

JIS G4305:2012 SUS312L: SUS312L: austenitic stainless steel, cold-rolled plate, sheet and strip. Specified in JIS G 4305:2012.

Category: Stainless Steel
Grade Details
GradeJIS G4305:2012 SUS312L
Standard JIS G4305:2012
ApplicationsCold-rolled stainless steel plates, sheet and strip
Equivalent / Similar Grades
Grade Standard Region Live on M-EX
ASTM A276/A276M S31254 ASTM A276/A276M:2017 USA No activity yet
EN 10088-1 X1CrNiMoCuN20-18-7 EN 10088-1:2014 Europe (CEN) No activity yet
JIS G4304 SUS312L JIS G4304:2021 Japan No activity yet
Grade ComparisonCompare With a Specific Grade →
Grade Standard Match
JIS G4304 SUS312L JIS G4304:2021 Strong Match
ASTM A276/A276M S31254 ASTM A276/A276M:2017 Strong Match
EN 10088-1 X1CrNiMoCuN20-18-7 EN 10088-1:2014 Strong Match
EN 10088-1 X1CrNiMoCuN20-18-7 EN 10088-1:2023 Strong Match
ASTM A959 S31254 ASTM A959:2011 Close Alternative
IS 6603 X01Cr20Ni18Mo6CuN IS 6603:2024 Close Alternative
EN 10088-3 X1CrNiMoCuN20-18-7 EN 10088-3:2014 Close Alternative
ASTM A240/A240M S31254 ASTM A240/A240M:2025 Close Alternative
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Chemical Composition (%)
C Si Mn P S Ni Cr Mo Cu N
<=0.020 <=0.80 <=1.00 <=0.030 <=0.015 17.50-19.50 19.00-21.00 6.00-7.00 0.50-1.00 0.16-0.25
Mechanical Properties
Tensile Strength >=650 MPa
Yield Strength >=300 MPa
Elongation >=35%
Hardness <=223 HB
Condition Solution heat treated plate and strip; 0.2 percent proof strength applies only when specified by the purchaser

More data from JIS G4305:2012

From the standard
Mechanical properties, solution heat treated 3 values
0.2 percent proof strength, min
300 MPa
Tensile strength, min
650 MPa
Elongation, min
35 %
0.2 percent proof strength applies only when specified by the purchaser. 1 N/mm2 = 1 MPa.
Source: JIS G 4305:2012, Table 8
Hardness, solution heat treated 3 scales
Brinell hardness HBW, max
223
Rockwell HRBW or HRBS, max
96
Vickers hardness HV, max
230
Any one of the hardness scales applies; if not specified the manufacturer selects. HRBW is used in case of dispute.
Source: JIS G 4305:2012, Table 8
Heat treatment (example, informative) 1 settings
Solution heat treatment
1010 to 1150 deg C, rapid cooling
Annex JA is informative; temperatures are examples.
Source: JIS G 4305:2012, Table JA.1

Active JIS G4305:2012 SUS312L Listings on M-EX (For Sale)

+ Create a Listing for this grade

No active JIS G4305:2012 SUS312L listings at this time.

Register for Alerts

Buyer RFQs for JIS G4305:2012 SUS312L

+ Post an RFQ for this grade

No open buyer requirements for JIS G4305:2012 SUS312L at this time.

Register for Alerts