JIS G4305 SUS312L vs JIS G4304 SUS312L

Strong Match — 100% match based on chemical composition and mechanical property overlap.

JIS G4305 SUS312L (JIS G4305:2012) and JIS G4304 SUS312L (JIS G4304:2021) are both steel grades. Both fall under the Stainless Steel category. JIS G4305 SUS312L is typically used for cold-rolled stainless steel plates, sheet and strip, while JIS G4304 SUS312L is commonly used for hot-rolled stainless steel plates and strips. JIS G4305 SUS312L is defined under Japanese Industrial Standards (JIS), originating from Japan, while JIS G4304 SUS312L is defined under Japanese Industrial Standards (JIS), originating from Japan.

As per chemical composition, JIS G4305 SUS312L vs JIS G4304 SUS312L is a 100% match. As per mechanical properties, the match is 100%. Combined, this makes them a strong match overall at 100%.

Frequently Compared With JIS G4305 SUS312L:
GOST 5632 06Kh23N28 EN 10088-1 1.4401 IS 1570 (Part 7) 12Cr12MoVH IS 1570 (Part 7) 12Cr13H ASTM A959 .- GB/T 3280 06Cr19Ni10 GOST 5632 08X18H10 EN 10088-1 1.4006 EN 10088-1 1.4301 EN 10088-1 1.4845 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoH
Match Breakdown
CHEMISTRY MATCH
100%
MECHANICAL MATCH
100%
OVERALL
100%
Specifications
Property JIS G4305 SUS312L JIS G4304 SUS312L
Standard JIS G4305:2012 JIS G4304:2021
Category Stainless Steel Stainless Steel
C (%) <=0.020 <=0.020
Si (%) <=0.80 <=0.80
Mn (%) <=1.00 <=1.00
P (%) <=0.030 <=0.030
S (%) <=0.015 <=0.015
Ni (%) 17.50-19.50 17.50-19.50
Cr (%) 19.00-21.00 19.00-21.00
Mo (%) 6.00-7.00 6.00-7.00
Cu (%) 0.50-1.00 0.50-1.00
N (%) 0.16-0.25 0.16-0.25
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property JIS G4305 SUS312L JIS G4304 SUS312L
Tensile Strength >=650 MPa >=650 MPa
Yield Strength >=300 MPa >=300 MPa
Elongation >=35% >=35%
Hardness <=223 HB <=223 HB
Condition Solution heat treated plate and strip; 0.2 percent proof strength applies only when specified by the purchaser Solution heat treated plate and strip; 0.2 percent proof strength applies only when specified by the purchaser
Typical Applications
JIS G4305 SUS312L
Cold-rolled stainless steel plates, sheet and strip
JIS G4304 SUS312L
Hot-rolled stainless steel plates and strips
Can JIS G4305 SUS312L Be Substituted With JIS G4304 SUS312L?
JIS G4305 SUS312L and JIS G4304 SUS312L overlap closely enough on chemistry and mechanical properties that JIS G4304 SUS312L is often considered as a substitute for JIS G4305 SUS312L in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
On M-EX Right Now
JIS G4305 SUS312L
0 active listings and RFQs →
JIS G4304 SUS312L
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between JIS G4305 SUS312L and JIS G4304 SUS312L?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can JIS G4305 SUS312L be substituted with JIS G4304 SUS312L?
JIS G4305 SUS312L and JIS G4304 SUS312L overlap closely enough on chemistry and mechanical properties that JIS G4304 SUS312L is often considered as a substitute for JIS G4305 SUS312L in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.