Minimal Match — 30.6% match
based on chemical composition and mechanical property overlap.
UNS C52100 and UNS C95400 are both bronze grades.
Both fall under the Bronze Alloys category.
UNS C52100 is defined under Unified Numbering System (UNS), originating from United States, while UNS C95400 is defined under Unified Numbering System (UNS), originating from United States.
As per chemical composition, UNS C52100 vs UNS C95400 is a 27.5% match.
As per mechanical properties, the match is 36.7%.
Combined, this makes them a minimal match overall at 30.6%.
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property
UNS C52100
UNS C95400
Yield Strength
~500-585 MPa (H02 half-hard)
~240-360 MPa (as cast)
Tensile Strength
~650-800 MPa (H02 half-hard)
~600-710 MPa (as cast)
Elongation
~8-18% (H02 half-hard)
~8-16% (as cast)
Note
Phosphor bronze 8% Sn, values for H02 half-hard temper, common spring stock
UNS C52100 specifies Pb, Sn, Zn, P which are not specified for UNS C95400.
UNS C95400 specifies Ni, Al, Mn which are not specified for UNS C52100.
Can UNS C52100 Be Substituted With UNS C95400?
UNS C52100 and UNS C95400 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
What is the difference between UNS C52100 and UNS C95400?
UNS C52100 specifies Pb, Sn, Zn, P which are not specified for UNS C95400. UNS C95400 specifies Ni, Al, Mn which are not specified for UNS C52100.
Can UNS C52100 be substituted with UNS C95400?
UNS C52100 and UNS C95400 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.