UNS C12000 Copper: Specifications & Listings

UNS C12000: DLP Copper (Phosphorus Deoxidized, Low P)

Category: Copper Alloys
Grade Details
GradeUNS C12000
Standard UNS
Equivalent / Similar Grades
Grade Standard Region Live on M-EX
EN CW023A (Cu-DLP) EN 1976 International Not yet on M-EX
JIS C1201 JIS H3100 International Not yet on M-EX
Grade ComparisonCompare With a Specific Grade →
Grade Standard Match
UNS C11000 UNS Strong Match
UNS C12200 UNS Strong Match
UNS C10200 UNS Strong Match
UNS C14500 UNS Related Material
UNS C10100 UNS Related Material
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Chemical Composition (%)
Cu P
99.90 min 0.004-0.012
Mechanical Properties
Yield Strength ~69 MPa (annealed O60)
Tensile Strength ~220 MPa (annealed O60)
Elongation ~45% (annealed O60)
Note Phosphorized copper (low P), values for soft annealed condition

Active UNS C12000 Listings on M-EX (For Sale)

+ Create a Listing for this grade

No active UNS C12000 listings at this time.

Register for Alerts

Buyer RFQs for UNS C12000

+ Post an RFQ for this grade

No open buyer requirements for UNS C12000 at this time.

Register for Alerts