Related Material — 66.2% match
based on chemical composition and mechanical property overlap.
AISI D2 KNL (ASTM A681) and ASTM A681 A5 (ASTM A681:2008) are both steel grades.
Both fall under the Tool & Die Steels category.
AISI D2 KNL is typically used for blanking dies, forming dies, thread rolling dies, punches, shear blades, gauges, broaches, drawing dies, while ASTM A681 A5 is commonly used for tools, dies and fixtures (clause 1.2).
AISI D2 KNL is defined under AISI, originating from United States, while ASTM A681 A5 is defined under ASTM International, originating from United States.
As per chemical composition, AISI D2 KNL vs ASTM A681 A5 is a 66.2% match.
Mechanical property data is not available for both grades, so this factor could not be scored.
Combined, this makes them a related material overall at 66.2%.
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property
AISI D2 KNL
ASTM A681 A5
Hardness (annealed)
≤255 HB
Not specified
Hardness (hardened)
58–62 HRC
Not specified
Compressive Strength
2600 MPa
Not specified
Typical Applications
AISI D2 KNL
Blanking dies, forming dies, thread rolling dies, punches, shear blades, gauges, broaches, drawing dies
ASTM A681 A5
Tools, dies and fixtures (clause 1.2)
Key Differences
AISI D2 KNL specifies V which is not specified for ASTM A681 A5.
Can AISI D2 KNL Be Substituted With ASTM A681 A5?
AISI D2 KNL and ASTM A681 A5 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
What is the difference between AISI D2 KNL and ASTM A681 A5?
AISI D2 KNL specifies V which is not specified for ASTM A681 A5.
Can AISI D2 KNL be substituted with ASTM A681 A5?
AISI D2 KNL and ASTM A681 A5 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.