ASTM A959 SS410 vs IS 6911 X04Cr12

Strong Match — 93.3% match based on chemical composition and mechanical property overlap.

ASTM A959 SS410 (ASTM A959:2011) and IS 6911 X04Cr12 (IS 6911:1992) are both steel grades. Both fall under the Stainless Steel category. ASTM A959 SS410 is typically used for cutlery, turbine blades, surgical instruments, fasteners, while IS 6911 X04Cr12 is commonly used for stainless and heat-resisting steel plate, sheet and strip (clause 1.1). ASTM A959 SS410 is defined under ASTM International, originating from United States, while IS 6911 X04Cr12 is defined under Bureau of Indian Standards (IS), originating from India.

As per chemical composition, ASTM A959 SS410 vs IS 6911 X04Cr12 is a 93.3% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a strong match overall at 93.3%.

Frequently Compared With ASTM A959 SS410:
EN 10088-1 1.4006 GOST 5632 12Kh13 GB/T 3280 06Cr19Ni10 EN 10088-1 1.4401 GOST 5632 06Kh23N28 EN 10088-1 1.4301 EN 10088-1 1.4845 GOST 5632 08X18H10 ASTM A959 .- IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoVH IS 1570 (Part 7) 12Cr12MoH
Match Breakdown
CHEMISTRY MATCH
93.3%
MECHANICAL MATCH
No shared data
OVERALL
93.3%
Specifications
Property ASTM A959 SS410 IS 6911 X04Cr12
Standard ASTM A959:2011 IS 6911:1992
Category Stainless Steel Stainless Steel
C (%) <=0.15 <=0.08
Cr (%) 11.5-13.5 11.5-13.5
Mn (%) <=1.00 <=1.0
P (%) <=0.040 <=0.040
S (%) <=0.030 <=0.030
Si (%) <=1.00 <=1.0
Al (%) Not specified 0.10-0.30
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property ASTM A959 SS410 IS 6911 X04Cr12
Bend Test (180 deg) Not specified Mandrel diameter 2 x thickness
Elongation (50 mm, annealed) Not specified >=20%
Hardness (annealed, max) Not specified 187 HBS, 88 HRB
Tensile Strength (annealed) Not specified >=440 MPa
Yield Strength (0.2% proof, annealed) Not specified >=250 MPa
Typical Applications
ASTM A959 SS410
Cutlery, turbine blades, surgical instruments, fasteners
IS 6911 X04Cr12
Stainless and heat-resisting steel plate, sheet and strip (clause 1.1)
Key Differences
Can ASTM A959 SS410 Be Substituted With IS 6911 X04Cr12?
ASTM A959 SS410 and IS 6911 X04Cr12 overlap closely enough on chemistry and mechanical properties that IS 6911 X04Cr12 is often considered as a substitute for ASTM A959 SS410 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
Forms & Sizes Available on M-EX
ASTM A959 SS410
Round Bar → (3 listings)
Diameter: 40–40 mm (1.57–1.57 in)
Length: 2800–3300 mm (110.24–129.92 in)
IS 6911 X04Cr12
No active listings currently.
On M-EX Right Now
ASTM A959 SS410
3 active listings and RFQs →
IS 6911 X04Cr12
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between ASTM A959 SS410 and IS 6911 X04Cr12?
IS 6911 X04Cr12 specifies Al which is not specified for ASTM A959 SS410.
Can ASTM A959 SS410 be substituted with IS 6911 X04Cr12?
ASTM A959 SS410 and IS 6911 X04Cr12 overlap closely enough on chemistry and mechanical properties that IS 6911 X04Cr12 is often considered as a substitute for ASTM A959 SS410 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.