AS/NZS 1595 C350 vs EN 10346 S350GD

Strong Match — 88.9% match based on chemical composition and mechanical property overlap.

AS/NZS 1595 C350 (AS/NZS 1595:1998) and EN 10346 S350GD (EN 10346:2015) are both steel grades. Both fall under the Structural Steel category. AS/NZS 1595 C350 is typically used for cold-rolled structural steel sheet; roll-forming, cold-formed structural sections, purlins, while EN 10346 S350GD is commonly used for continuous hot-dip galvanized structural steel strip/sheet; roll-formed and cold-formed structural sections, purlins, roofing and cladding requiring corrosion protection. AS/NZS 1595 C350 is defined under Australian/New Zealand Standard (AS/NZS), originating from Australia/New Zealand, while EN 10346 S350GD is defined under European Standard (EN), originating from Europe.

As per chemical composition, AS/NZS 1595 C350 vs EN 10346 S350GD is a 100% match. As per mechanical properties, the match is 66.7%. Combined, this makes them a strong match overall at 88.9%.

Frequently Compared With AS/NZS 1595 C350:
CSA G40.21 480W CSA G40.21 300W CSA G40.21 350W ASTM A1008 SS Grade 50 AS/NZS 3679.1 300 CSA G40.21 400A GOST 19281 09G2S CSA G40.21 260W CSA G40.21 400W AS/NZS 3679.1 350 ASTM A1008 SS Grade 80 ASTM A283C
Match Breakdown
CHEMISTRY MATCH
100%
MECHANICAL MATCH
66.7%
OVERALL
88.9%
Specifications
Property AS/NZS 1595 C350 EN 10346 S350GD
Standard AS/NZS 1595:1998 EN 10346:2015
Category Structural Steel Structural Steel
C (%) <=0.20 <=0.20
Mn (%) <=1.50 <=1.50
Si (%) <=0.50 <=0.50
P (%) <=0.040 <=0.040
S (%) <=0.040 <=0.040
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property AS/NZS 1595 C350 EN 10346 S350GD
Tensile Strength 430 MPa min 420 MPa min
Yield Strength 350 MPa min 350 MPa min
Elongation 14% min 14% min
Typical Applications
AS/NZS 1595 C350
Cold-rolled structural steel sheet; roll-forming, cold-formed structural sections, purlins
EN 10346 S350GD
Continuous hot-dip galvanized structural steel strip/sheet; roll-formed and cold-formed structural sections, purlins, roofing and cladding requiring corrosion protection
Can AS/NZS 1595 C350 Be Substituted With EN 10346 S350GD?
AS/NZS 1595 C350 and EN 10346 S350GD overlap closely enough on chemistry and mechanical properties that EN 10346 S350GD is often considered as a substitute for AS/NZS 1595 C350 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
Forms & Sizes Available on M-EX
AS/NZS 1595 C350
Plate → (2 listings)
Thickness: 10–10 mm (0.39–0.39 in)
Width: 1500–1500 mm (59.06–59.06 in)
Length: 2500–4600 mm (98.43–181.1 in)
EN 10346 S350GD
Plate → (2 listings)
Thickness: 10–10 mm (0.39–0.39 in)
Width: 1500–1500 mm (59.06–59.06 in)
Length: 2700–4100 mm (106.3–161.42 in)
On M-EX Right Now
AS/NZS 1595 C350
2 active listings and RFQs →
EN 10346 S350GD
2 active listings and RFQs →
Frequently Asked Questions
What is the difference between AS/NZS 1595 C350 and EN 10346 S350GD?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can AS/NZS 1595 C350 be substituted with EN 10346 S350GD?
AS/NZS 1595 C350 and EN 10346 S350GD overlap closely enough on chemistry and mechanical properties that EN 10346 S350GD is often considered as a substitute for AS/NZS 1595 C350 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.