Related Material — 65.4% match
based on chemical composition and mechanical property overlap.
AS/NZS 3679.1 300 (AS/NZS 3679.1:2016) and ASTM A1008 SS Grade 50 (ASTM A1008) are both steel grades.
Both fall under the Structural Steel category.
AS/NZS 3679.1 300 is typically used for hot-rolled structural bars and sections for general structural framing, while ASTM A1008 SS Grade 50 is commonly used for cold-rolled high-strength structural steel sheet; automotive structural components, cold-formed parts requiring moderate strength.
AS/NZS 3679.1 300 is defined under Australian/New Zealand Standard (AS/NZS), originating from Australia/New Zealand, while ASTM A1008 SS Grade 50 is defined under ASTM International, originating from United States.
As per chemical composition, AS/NZS 3679.1 300 vs ASTM A1008 SS Grade 50 is a 98% match.
As per mechanical properties, the match is 0%.
Combined, this makes them a related material overall at 65.4%.
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property
AS/NZS 3679.1 300
ASTM A1008 SS Grade 50
Tensile Strength
440-600 MPa
380 MPa min
Yield Strength
300 MPa min
340 MPa min
Elongation
22% min
14% min
Typical Applications
AS/NZS 3679.1 300
Hot-rolled structural bars and sections for general structural framing
Can AS/NZS 3679.1 300 Be Substituted With ASTM A1008 SS Grade 50?
AS/NZS 3679.1 300 and ASTM A1008 SS Grade 50 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
What is the difference between AS/NZS 3679.1 300 and ASTM A1008 SS Grade 50?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can AS/NZS 3679.1 300 be substituted with ASTM A1008 SS Grade 50?
AS/NZS 3679.1 300 and ASTM A1008 SS Grade 50 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.