ASTM A276/A276M S24000 vs ASTM A276/A276M S24100

Strong Match — 88.8% match based on chemical composition and mechanical property overlap.

ASTM A276/A276M S24000 (ASTM A276/A276M:2017) and ASTM A276/A276M S24100 (ASTM A276/A276M:2017) are both steel grades. Both fall under the Stainless Steel category. ASTM A276/A276M S24000 is typically used for stainless steel bars and shapes (hot-finished or cold-finished), while ASTM A276/A276M S24100 is commonly used for stainless steel bars and shapes (hot-finished or cold-finished). ASTM A276/A276M S24000 is defined under ASTM International, originating from United States, while ASTM A276/A276M S24100 is defined under ASTM International, originating from United States.

As per chemical composition, ASTM A276/A276M S24000 vs ASTM A276/A276M S24100 is a 83.2% match. As per mechanical properties, the match is 100%. Combined, this makes them a strong match overall at 88.8%.

Frequently Compared With ASTM A276/A276M S24000:
ASTM A959 .- IS 1570 (Part 7) 11Cr17Ni13W3TiH EN 10088-1 1.4006 EN 10088-1 1.4401 EN 10088-1 1.4845 IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12Ni2Mo GB/T 3280 06Cr19Ni10 GOST 5632 06Kh23N28 GOST 5632 08X18H10 EN 10088-1 1.4301 IS 1570 (Part 7) 12Cr12MoVH
Match Breakdown
CHEMISTRY MATCH
83.2%
MECHANICAL MATCH
100%
OVERALL
88.8%
Specifications
Property ASTM A276/A276M S24000 ASTM A276/A276M S24100
Standard ASTM A276/A276M:2017 ASTM A276/A276M:2017
Category Stainless Steel Stainless Steel
C (%) <=0.08 <=0.15
Mn (%) 11.5-14.5 11.0-14.0
P (%) <=0.060 <=0.045
S (%) <=0.030 <=0.030
Si (%) <=1.00 <=1.00
Cr (%) 17.0-19.0 16.5-19.0
Ni (%) 2.3-3.7 0.50-2.50
N (%) 0.20-0.40 0.20-0.45
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property ASTM A276/A276M S24000 ASTM A276/A276M S24100
Tensile Strength >=690 MPa >=690 MPa
Yield Strength >=380 MPa >=380 MPa
Elongation >=30% >=30%
Condition Condition A (Annealed), hot-finished or cold-finished, all sizes (first row printed) Condition A (Annealed), hot-finished or cold-finished, all sizes (first row printed)
Typical Applications
ASTM A276/A276M S24000
Stainless steel bars and shapes (hot-finished or cold-finished)
ASTM A276/A276M S24100
Stainless steel bars and shapes (hot-finished or cold-finished)
Can ASTM A276/A276M S24000 Be Substituted With ASTM A276/A276M S24100?
ASTM A276/A276M S24000 and ASTM A276/A276M S24100 overlap closely enough on chemistry and mechanical properties that ASTM A276/A276M S24100 is often considered as a substitute for ASTM A276/A276M S24000 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
On M-EX Right Now
ASTM A276/A276M S24000
0 active listings and RFQs →
ASTM A276/A276M S24100
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between ASTM A276/A276M S24000 and ASTM A276/A276M S24100?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can ASTM A276/A276M S24000 be substituted with ASTM A276/A276M S24100?
ASTM A276/A276M S24000 and ASTM A276/A276M S24100 overlap closely enough on chemistry and mechanical properties that ASTM A276/A276M S24100 is often considered as a substitute for ASTM A276/A276M S24000 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.