ASTM A959 .- vs GOST 5632 12Kh13

Minimal Match — 35% match based on chemical composition and mechanical property overlap.

ASTM A959 .- (ASTM A959:2011) and GOST 5632 12Kh13 (GOST 5632-2014) are both steel grades. Both fall under the Stainless Steel category. ASTM A959 .- is typically used for wrought stainless steel products; recommended composition limits for adoption by product standards (clause 1.1), while GOST 5632 12Kh13 is commonly used for turbine blades, pump shafts, fasteners, cutlery. ASTM A959 .- is defined under ASTM International (United States).

As per chemical composition, ASTM A959 .- vs GOST 5632 12Kh13 is a 55.8% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a minimal match overall at 35%.

Frequently Compared With ASTM A959 .-:
ASTM A959 201L ASTM A959 202 ASTM A959 16-8-2H ASTM A959 201 ASTM A959 201LN EN 10088-1 1.4301 ASTM A959 29-4 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12Ni2Mo GB/T 3280 06Cr19Ni10 GOST 5632 08X18H10 GOST 5632 06Kh23N28
Match Breakdown
CHEMISTRY MATCH
55.8%
MECHANICAL MATCH
No shared data
OVERALL
35%
Specifications
Property ASTM A959 .- GOST 5632 12Kh13
Standard ASTM A959:2011 GOST 5632-2014
Category Stainless Steel Stainless Steel
C (%) <=0.030 0.09–0.15
Cb (%) 0.10-0.60 Not specified
Cr (%) 18.0-20.0 12.0–14.0
Mn (%) <=1.00 ≤0.80
N (%) <=0.030 Not specified
Ni (%) <=0.50 ≤0.60
P (%) <=0.040 Not specified
S (%) <=0.030 Not specified
Si (%) <=1.00 ≤0.80
Ti (%) 0.07-0.30 Not specified
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property ASTM A959 .- GOST 5632 12Kh13
Tensile Strength Not specified ≥540 MPa (annealed)
Hardness HRC Not specified 36–45 (hardened)
Typical Applications
ASTM A959 .-
Wrought stainless steel products; recommended composition limits for adoption by product standards (clause 1.1)
GOST 5632 12Kh13
Turbine blades, pump shafts, fasteners, cutlery
Key Differences
Can ASTM A959 .- Be Substituted With GOST 5632 12Kh13?
ASTM A959 .- and GOST 5632 12Kh13 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
Forms & Sizes Available on M-EX
ASTM A959 .-
No active listings currently.
GOST 5632 12Kh13
Sheet → (2 listings)
Thickness: 6–6 mm (0.24–0.24 in)
Width: 1250–1250 mm (49.21–49.21 in)
Length: 2700–3400 mm (106.3–133.86 in)
On M-EX Right Now
ASTM A959 .-
0 active listings and RFQs →
GOST 5632 12Kh13
2 active listings and RFQs →
Frequently Asked Questions
What is the difference between ASTM A959 .- and GOST 5632 12Kh13?
ASTM A959 .- specifies Cb, N, P, S which are not specified for GOST 5632 12Kh13.
Can ASTM A959 .- be substituted with GOST 5632 12Kh13?
ASTM A959 .- and GOST 5632 12Kh13 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.