ASTM A959:2011 2507: Duplex (austenitic-ferritic) stainless steel type 2507 (UNS S32750) with the composition limits of ASTM A959-11. Carbon up to 0.030% and chromium 24.0-26.0%.
| Grade | ASTM A959:2011 2507 |
| Standard | ASTM A959:2011 |
| Applications | Wrought stainless steel products; recommended composition limits for adoption by product standards (clause 1.1) |
| Grade | Standard | Region | Live on M-EX |
|---|---|---|---|
| ASTM A240/A240M S32750 | ASTM A240/A240M:2025 | USA | No activity yet |
| JIS G4304 SUS327L1 | JIS G4304:2021 | Japan | No activity yet |
| IS 6603 X02Cr25Ni7Mo4N | IS 6603:2024 | India | No activity yet |
| EN 10088-1 X2CrNiMoN25-7-4 | EN 10088-1:2014 | Europe (CEN) | No activity yet |
| EN 10088-3 X2CrNiMoN25-7-4 | EN 10088-3:2014 | Europe | No activity yet |
| ASTM A240/A240M S32520 | ASTM A240/A240M:2025 | USA | No activity yet |
| EN 10088-1 X2CrNiMoCuN25-6-3 | EN 10088-1:2014 | Europe (CEN) | No activity yet |
| EN 10088-3 X2CrNiMoCuN25-6-3 | EN 10088-3:2014 | Europe | No activity yet |
| Grade | Standard | Match |
|---|---|---|
| ASTM A240/A240M S32750 | ASTM A240/A240M:2025 | Strong Match |
| ASTM A276/A276M S32750 | ASTM A276/A276M:2017 | Strong Match |
| JIS G4304 SUS327L1 | JIS G4304:2021 | Strong Match |
| ASTM A959 S32520 | ASTM A959:2011 | Strong Match |
| IS 6603 X02Cr25Ni7Mo4N | IS 6603:2024 | Strong Match |
| EN 10088-1 X2CrNiMoN25-7-4 | EN 10088-1:2014 | Strong Match |
| EN 10088-1 X2CrNiMoN25-7-4 | EN 10088-1:2023 | Strong Match |
| EN 10088-3 X2CrNiMoN25-7-4 | EN 10088-3:2014 | Strong Match |
| C | Cr | Cu | Mn | Mo | N | Ni | P | S | Si |
|---|---|---|---|---|---|---|---|---|---|
| <=0.030 | 24.0-26.0 | <=0.50 | <=1.20 | 3.0-5.0 | 0.24-0.32 | 6.0-8.0 | <=0.035 | <=0.020 | <=0.80 |