ASTM A959:2011 316L Steel: Specifications & Listings

ASTM A959:2011 316L: Austenitic stainless steel type 316L (UNS S31603) with the composition limits of ASTM A959-11. Carbon up to 0.030% and chromium 16.0-18.0%.

Category: Stainless Steel
Grade Details
GradeASTM A959:2011 316L
Standard ASTM A959:2011
ApplicationsWrought stainless steel products; recommended composition limits for adoption by product standards (clause 1.1)
Equivalent / Similar Grades
Grade Standard Region Live on M-EX
IS 1570 (Part 7) 3Cr17Ni12Mo3H IS 1570 (Part 7):1992 India No activity yet
IS 1570 (Part 5) X02Cr17Ni12Mo2 IS 1570 (Part 5):1985 India No activity yet
ASTM A276/A276M S31603 ASTM A276/A276M:2017 USA No activity yet
JIS G4304 SUS316L JIS G4304:2021 Japan No activity yet
BS 970 (Part 1) 316S11 BS 970 (Part 1):1991 UK No activity yet
BS 970 (Part 1) 316S13 BS 970 (Part 1):1991 UK No activity yet
ASTM A240/A240M S31653 ASTM A240/A240M:2025 USA No activity yet
ASTM A276/A276M S31654 ASTM A276/A276M:2017 USA No activity yet
IS 6603 X02Cr17Ni12Mo2N IS 6603:2024 India No activity yet
EN 10088-3 X2CrNiMo17-12-2 EN 10088-3:2014 Europe No activity yet
EN 10088-3 X2CrNiMo17-12-3 EN 10088-3:2014 Europe No activity yet
JIS G4304 SUS316LN JIS G4304:2021 Japan No activity yet
Grade ComparisonCompare With a Specific Grade →
Grade Standard Match
IS 1570 (Part 5) X02Cr17Ni12Mo2 IS 1570 (Part 5):1985 Strong Match
IS 1570 (Part 7) 3Cr17Ni12Mo3H IS 1570 (Part 7):1992 Strong Match
IS 11169 (Part 2) X02Cr17Ni12Mo2 IS 11169 (Part 2):1989 Strong Match
IS 6911 X02Cr17Ni12Mo2 IS 6911:1992 Strong Match
ASTM A276/A276M S31603 ASTM A276/A276M:2017 Strong Match
ASTM A240/A240M S31603 ASTM A240/A240M:2025 Strong Match
IS 6603 X02Cr17Ni12Mo2 IS 6603:2024 Strong Match
JIS G4304 SUS316L JIS G4304:2021 Strong Match
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Chemical Composition (%)
C Cr Mn Mo Ni P S Si
<=0.030 16.0-18.0 <=2.00 2.00-3.00 10.0-14.0 <=0.045 <=0.030 <=1.00

More data from ASTM A959:2011

From the standard
Other composition limits from Table 1 and its footnotes
UNS number
S31603
Metallurgical class
Austenitic grade: usually predominantly face-centered cubic, hardenable only by cold working
Type
316L (designation originally assigned by the American Iron and Steel Institute)
Values
Maximum unless a range or minimum is shown; where two limits are shown for the same element in one grade the more stringent applies
These are the recommended composition limits of the A959 guide, intended for adoption by standards for stainless steel products; they are not a product specification.
Source: ASTM A959:2011, Table 1 and its footnotes

Active ASTM A959:2011 316L Listings on M-EX (For Sale)

+ Create a Listing for this grade

No active ASTM A959:2011 316L listings at this time.

Register for Alerts

Buyer RFQs for ASTM A959:2011 316L

+ Post an RFQ for this grade

No open buyer requirements for ASTM A959:2011 316L at this time.

Register for Alerts