ASTM A959:2011 429: Ferritic stainless steel type 429 (UNS S42900) with the composition limits of ASTM A959-11. Carbon up to 0.12% and chromium 14.0-16.0%.
| Grade | ASTM A959:2011 429 |
| Standard | ASTM A959:2011 |
| Applications | Wrought stainless steel products; recommended composition limits for adoption by product standards (clause 1.1) |
| Grade | Standard | Region | Live on M-EX |
|---|---|---|---|
| ASTM A240/A240M S42900 | ASTM A240/A240M:2025 | USA | No activity yet |
| ASTM A276/A276M S43000 | ASTM A276/A276M:2017 | USA | No activity yet |
| IS 11169 (Part 2) X07Cr17 | IS 11169 (Part 2):1989 | India | No activity yet |
| IS 1570 (Part 5) X04Cr12 | IS 1570 (Part 5):1985 | India | No activity yet |
| IS 11169 (Part 2) X04Cr17 | IS 11169 (Part 2):2023 | India | No activity yet |
| EN 10088-3 X6Cr13 | EN 10088-3:2014 | Europe | No activity yet |
| EN 10088-1 X6Cr17 | EN 10088-1:2014 | Europe (CEN) | No activity yet |
| EN 10088-3 X6Cr17 | EN 10088-3:2014 | Europe | No activity yet |
| Grade | Standard | Match |
|---|---|---|
| ASTM A240/A240M S42900 | ASTM A240/A240M:2025 | Strong Match |
| ASTM A276/A276M S42900 | ASTM A276/A276M:2017 | Strong Match |
| ASTM A959 430 | ASTM A959:2011 | Strong Match |
| ASTM A276/A276M S43000 | ASTM A276/A276M:2017 | Strong Match |
| IS 11169 (Part 2) X07Cr17 | IS 11169 (Part 2):1989 | Strong Match |
| ASTM A959 SS410 | ASTM A959:2011 | Strong Match |
| IS 1570 (Part 5) X04Cr12 | IS 1570 (Part 5):1985 | Strong Match |
| IS 11169 (Part 2) X04Cr17 | IS 11169 (Part 2):2023 | Strong Match |
| C | Cr | Mn | P | S | Si |
|---|---|---|---|---|---|
| <=0.12 | 14.0-16.0 | <=1.00 | <=0.040 | <=0.030 | <=1.00 |