ASTM A959 616 vs EN 10088-1 X20CrMoV11-1

Close Alternative — 72.7% match based on chemical composition and mechanical property overlap.

ASTM A959 616 (ASTM A959:2011) and EN 10088-1 X20CrMoV11-1 (EN 10088-1:2014) are both steel grades. Both fall under the Stainless Steel category. ASTM A959 616 is defined under ASTM International, originating from United States, while EN 10088-1 X20CrMoV11-1 is defined under European Standard (EN), originating from Europe.

As per chemical composition, ASTM A959 616 vs EN 10088-1 X20CrMoV11-1 is a 72.7% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a close alternative overall at 72.7%.

Frequently Compared With ASTM A959 616:
IS 1570 (Part 7) 20Cr12MoNiVH EN 10088-1 1.4845 IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12Ni2Mo GOST 5632 08X18H10 ASTM A959 .- GB/T 3280 06Cr19Ni10 GOST 5632 06Kh23N28 EN 10088-1 1.4006 EN 10088-1 1.4401 EN 10088-1 1.4301 IS 1570 (Part 7) 11Cr17Ni13W3TiH
Match Breakdown
CHEMISTRY MATCH
72.7%
MECHANICAL MATCH
No shared data
OVERALL
72.7%
Specifications
Property ASTM A959 616 EN 10088-1 X20CrMoV11-1
Standard ASTM A959:2011 EN 10088-1:2014
Category Stainless Steel Stainless Steel
C (%) 0.20-0.25 0.17-0.23
Cr (%) 11.0-12.5 10.0-12.5
Mn (%) 0.50-1.00 0.30-1.00
Mo (%) 0.90-1.25 0.80-1.20
Ni (%) 0.50-1.00 0.30-0.80
P (%) <=0.025 <=0.025
S (%) <=0.025 <=0.015
Si (%) <=0.50 <=0.40
V (%) 0.20-0.30 0.20-0.35
W (%) 0.90-1.25 Not specified
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Typical Applications
ASTM A959 616
Wrought stainless steel products; recommended composition limits for adoption by product standards (clause 1.1)
EN 10088-1 X20CrMoV11-1
Not documented
Key Differences
Can ASTM A959 616 Be Substituted With EN 10088-1 X20CrMoV11-1?
ASTM A959 616 and EN 10088-1 X20CrMoV11-1 are a close alternative rather than a direct substitute. Some properties overlap well, but check the specific chemistry and mechanical rows above against your application's requirements before treating them as interchangeable.
On M-EX Right Now
ASTM A959 616
0 active listings and RFQs →
EN 10088-1 X20CrMoV11-1
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between ASTM A959 616 and EN 10088-1 X20CrMoV11-1?
ASTM A959 616 specifies W which is not specified for EN 10088-1 X20CrMoV11-1.
Can ASTM A959 616 be substituted with EN 10088-1 X20CrMoV11-1?
ASTM A959 616 and EN 10088-1 X20CrMoV11-1 are a close alternative rather than a direct substitute. Some properties overlap well, but check the specific chemistry and mechanical rows above against your application's requirements before treating them as interchangeable.