ASTM A959:2011 S30430: Austenitic stainless steel grade (UNS S30430) with the composition limits of ASTM A959-11. Carbon up to 0.03% and chromium 17.0-19.0%.
| Grade | ASTM A959:2011 S30430 |
| Standard | ASTM A959:2011 |
| Applications | Wrought stainless steel products; recommended composition limits for adoption by product standards (clause 1.1) |
| Grade | Standard | Region | Live on M-EX |
|---|---|---|---|
| IS 1570 (Part 7) 3Cr18Ni11H | IS 1570 (Part 7):1992 | India | No activity yet |
| IS 6603 X03Cr18Ni9Cu4 | IS 6603:2024 | India | No activity yet |
| IS 11169 (Part 2) X02Cr18Ni9Cu3 | IS 11169 (Part 2):2023 | India | No activity yet |
| EN 10088-3 X3CrNiCu18-9-4 | EN 10088-3:2014 | Europe | No activity yet |
| IS 11169 (Part 2) X02Cr19Ni9 | IS 11169 (Part 2):2023 | India | No activity yet |
| BS 970 (Part 1) 304S11 | BS 970 (Part 1):1991 | UK | No activity yet |
| EN 10088-1 X3CrNiCu18-9-4 | EN 10088-1:2014 | Europe (CEN) | No activity yet |
| EN 10088-3 X2CrNi18-9 | EN 10088-3:2014 | Europe | No activity yet |
| JIS G4304 SUS304LN | JIS G4304:2021 | Japan | No activity yet |
| Grade | Standard | Match |
|---|---|---|
| IS 6603 X03Cr18Ni9Cu4 | IS 6603:2024 | Strong Match |
| IS 11169 (Part 2) X02Cr18Ni9Cu3 | IS 11169 (Part 2):2023 | Strong Match |
| EN 10088-3 X3CrNiCu18-9-4 | EN 10088-3:2014 | Strong Match |
| IS 11169 (Part 2) X02Cr19Ni9 | IS 11169 (Part 2):2023 | Strong Match |
| BS 970 (Part 1) 304S11 | BS 970 (Part 1):1991 | Strong Match |
| BS 970 (Part 3) 304S11 | BS 970 (Part 3):1991 | Strong Match |
| BS 970 (Part 1) 304S11 | BS 970 (Part 1):1983 | Strong Match |
| IS 1570 (Part 7) 3Cr18Ni11H | IS 1570 (Part 7):1992 | Strong Match |
| C | Cr | Cu | Mn | Ni | P | S | Si |
|---|---|---|---|---|---|---|---|
| <=0.03 | 17.0-19.0 | 3.0-4.0 | <=2.00 | 8.0-10.0 | <=0.045 | <=0.030 | <=1.00 |