BS 970 (Part 1):1983 225M36 Steel: Specifications & Listings

BS 970 (Part 1):1983 225M36: 225M36 is a carbon manganese free-cutting steel grade specified in BS 970 Part 1:1983 (Table 6, category 2). Section three of the standard advises that category 1 steels be used for new designs and established designs whenever possible.

Category: Free Machining Steel
Grade Details
GradeBS 970 (Part 1):1983 225M36
Standard BS 970 (Part 1):1983
ApplicationsThrough hardening steel for mechanical and allied engineering purposes; supplied in the hardened and tempered conditions of Table 6.
Equivalent / Similar Grades
Grade Standard Region Live on M-EX
BS 970 (Part 3) 226M44 BS 970 (Part 3):1991 UK No activity yet
IS 1570 (Part 3) 40C10S18 IS 1570 (Part 3):1979 India No activity yet
BS 970 (Part 1) 212M36 BS 970 (Part 1):1983 UK No activity yet
BS 970 (Part 1) 212A37 BS 970 (Part 1):1983 UK No activity yet
BS 970 (Part 3) 216M36 BS 970 (Part 3):1991 UK No activity yet
BS 970 EN8M BS 970:1955 UK 3 listings, 0 RFQs →
Grade ComparisonCompare With a Specific Grade →
Grade Standard Match
BS 970 (Part 1) 212M36 BS 970 (Part 1):1983 Strong Match
BS 970 (Part 1) 212A37 BS 970 (Part 1):1983 Strong Match
BS 970 (Part 3) 216M36 BS 970 (Part 3):1991 Strong Match
BS 970 (Part 1) 216M36 BS 970 (Part 1):1983 Strong Match
BS 970 EN8M BS 970:1955 Strong Match
BS 970 (Part 3) 226M44 BS 970 (Part 3):1991 Strong Match
BS 970 (Part 1) 226M44 BS 970 (Part 1):1983 Strong Match
BS 970 EN15AM BS 970:1955 Strong Match
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Chemical Composition (%)
C Mn Si P S
0.32-0.40 1.00-1.40 <=0.25 <=0.060 0.20-0.30

More data from BS 970 (Part 1):1983

From the standard
Heat treatment and maximum hardness (through hardening)
Hardening temperature
840-870 deg C
Quenching medium
Oil
Tempering temperature
550-660 deg C
Hardenability test
No hardenability data specified
Softened condition
Not usually supplied in the softened condition
Heat treatment to be given to test bars and to material required in the finally heat treated condition. Note 24: O = oil, W = water. Where oil hardening is specified, either a well-agitated conventional oil or a proven synthetic quenchant may be used. Synthetic quenchants shall not be used for the heat treatment of test bars for material not supplied in the finally heat treated condition.
Source: BS 970 (Part 1):1983, Table 7
Mechanical properties by heat treatment condition
ConditionLimiting ruling section (mm)Rm (N/mm2)Re min (N/mm2)A min (%)Izod min (ft lbf)KCV min (J)Rp0.2 min (N/mm2), when specifically orderedHB
Q63625-775400182528370179-229
R13700-850480162528450201-255
Values as printed in Table 6 for the limiting ruling section shown. Rp0.2 applies when specifically ordered (note 10). 1 N/mm2 = 1 MPa.
Source: BS 970 (Part 1):1983, Table 6
Comparison with earlier editions
BS 970:1970/72 designation
225M36
BS 970:1955 En No.
None
Appendix D note 47: where a comparison is made the steels are not necessarily equivalent. 'Not listed' means the earlier edition has no entry under this designation.
Source: BS 970 (Part 1):1983, Appendix D

Active BS 970 (Part 1):1983 225M36 Listings on M-EX (For Sale)

+ Create a Listing for this grade

No active BS 970 (Part 1):1983 225M36 listings at this time.

Register for Alerts

Buyer RFQs for BS 970 (Part 1):1983 225M36

+ Post an RFQ for this grade

No open buyer requirements for BS 970 (Part 1):1983 225M36 at this time.

Register for Alerts