BS 970:1955 EN22 Steel: Specifications & Listings

BS 970:1955 EN22: EN22: 3 1/4 per cent nickel steel. Specified in BS 970:1955, Part 2.

Category: Alloy Steel
Grade Details
GradeBS 970:1955 EN22
Standard BS 970:1955
ApplicationsBars and billets for forging; forgings and drop-forgings; bars for machining; bright bars. Suitable for 50/60 (S) and 55/65 (T) tons/sq in according to ruling section.
Grade ComparisonCompare With a Specific Grade →
Grade Standard Match
BS 970 (Part 3) 635M15 BS 970 (Part 3):1991 Related Material
BS 970 (Part 3) 637M17 BS 970 (Part 3):1991 Related Material
BS 970 (Part 3) 655M13 BS 970 (Part 3):1991 Related Material
BS 970 EN111A BS 970:1955 Related Material
BS 970 (Part 1) 655H13 BS 970 (Part 1):1991 Related Material
SAE J404 50B46 SAE J404:2009 Related Material
IS 1570 (Part 4) 15Cr6Ni6 IS 1570 (Part 4):1988 Related Material
BS 970 (Part 1) 655M13 BS 970 (Part 1):1983 Related Material
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Chemical Composition (%)
C Si Mn Ni Cr S P
0.35-0.45 0.10-0.35 0.50-0.80 3.25-3.75 <=0.30 <=0.050 <=0.050
Mechanical Properties
Tensile Strength ≥772 MPa (50 tons/sq in, converted)
Yield Strength ≥587 MPa (38 tons/sq in, converted)
Elongation ≥20%
Hardness 223-277 HB
Condition Hardened and tempered S, ruling section 4 in (lowest-strength condition of the standard)

More data from BS 970:1955

From the standard
Condition of material on delivery
A
Bars and billets for forging as rolled or forged unless order states otherwise.
B
Forgings and drop-forgings finally heat treated unless order states otherwise.
C
Bars for machining finally heat treated unless order states otherwise.
D
Bright bars finally heat treated, before or after cold work at manufacturer option, unless order states otherwise.
Source: BS 970:1955, Part 2, En 22 (page 100)
Mechanical properties
ConditionRuling section or size (in)Tensile strength (tons/sq in)Yield stress (tons/sq in)Elongation (%)Izod impact (ft lb)Brinell (HB)Proof stress 0.2% (tons/sq in), when requested
Hardened and tempered S450382040223-27736
Hardened and tempered T2 1/255441840248-30241
Values as printed in BS 970:1955; tensile strength, yield stress and proof stress in tons/sq in, Izod in ft lb. Minimum unless a range is shown.
Source: BS 970:1955, Part 2, En 22 (page 101)
Heat treatment
Harden (oil)
830/860 C
Temper
suitable temperature between 550 C and 650 C
Temperatures in degrees C as printed.
Source: BS 970:1955, Part 2, En 22 (page 100)
Status in the 1955 edition
Status
Deleted by Amendment 7
Reason
Amendment 7 (Sep 1970): direct hardening alloy steels moved to BS 970 Part 2:1970
BS 970:1955 was amended up to Amendment 10 (June 1972); steels were moved to the revised Parts 1 to 5 and deleted from this edition.
Source: BS 970:1955, Amendment slips 6 to 10

Active BS 970:1955 EN22 Listings on M-EX (For Sale)

+ Create a Listing for this grade

No active BS 970:1955 EN22 listings at this time.

Register for Alerts

Buyer RFQs for BS 970:1955 EN22

+ Post an RFQ for this grade

No open buyer requirements for BS 970:1955 EN22 at this time.

Register for Alerts