CSA G40.21 300W vs AS/NZS 1595 C350

Related Material — 62.1% match based on chemical composition and mechanical property overlap.

CSA G40.21 300W (CSA G40.21-13 (R2023)) and AS/NZS 1595 C350 (AS/NZS 1595:1998) are both steel grades. Both fall under the Structural Steel category. CSA G40.21 300W is typically used for structural fabrication,bridges,buildings,machinery frames,general construction,welded structures, while AS/NZS 1595 C350 is commonly used for cold-rolled structural steel sheet; roll-forming, cold-formed structural sections, purlins. CSA G40.21 300W is defined under Canadian Standards Association (CSA), originating from Canada, while AS/NZS 1595 C350 is defined under Australian/New Zealand Standard (AS/NZS), originating from Australia/New Zealand.

As per chemical composition, CSA G40.21 300W vs AS/NZS 1595 C350 is a 93.2% match. As per mechanical properties, the match is 0%. Combined, this makes them a related material overall at 62.1%.

Frequently Compared With CSA G40.21 300W:
CSA G40.21 400W ASTM A1008 SS Grade 50 CSA G40.21 480W GOST 19281 09G2S CSA G40.21 400A AS/NZS 1595 C450 CSA G40.21 260W ASTM A572 Grade 50 IS 2062 E250A IS 2062 E250B0 ASTM A572 Gr.65 ASTM A283C
Match Breakdown
CHEMISTRY MATCH
93.2%
MECHANICAL MATCH
0%
OVERALL
62.1%
Specifications
Property CSA G40.21 300W AS/NZS 1595 C350
Standard CSA G40.21-13 (R2023) AS/NZS 1595:1998
Category Structural Steel Structural Steel
C (%) <=0.23 <=0.20
Mn (%) <=1.50 <=1.50
P (%) <=0.040 <=0.040
S (%) <=0.050 <=0.040
Si (%) Not specified <=0.50
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property CSA G40.21 300W AS/NZS 1595 C350
Tensile Strength 450-620 MPa 430 MPa min
Yield Strength 300 MPa min 350 MPa min
Elongation 20-23 % 14% min
Typical Applications
CSA G40.21 300W
structural fabrication,bridges,buildings,machinery frames,general construction,welded structures
AS/NZS 1595 C350
Cold-rolled structural steel sheet; roll-forming, cold-formed structural sections, purlins
Key Differences
Can CSA G40.21 300W Be Substituted With AS/NZS 1595 C350?
CSA G40.21 300W and AS/NZS 1595 C350 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
Forms & Sizes Available on M-EX
CSA G40.21 300W
Plate → (2 listings)
Thickness: 10–10 mm (0.39–0.39 in)
Width: 1500–1500 mm (59.06–59.06 in)
Length: 2700–2800 mm (106.3–110.24 in)
AS/NZS 1595 C350
Plate → (2 listings)
Thickness: 10–10 mm (0.39–0.39 in)
Width: 1500–1500 mm (59.06–59.06 in)
Length: 2500–4600 mm (98.43–181.1 in)
On M-EX Right Now
CSA G40.21 300W
2 active listings and RFQs →
AS/NZS 1595 C350
2 active listings and RFQs →
Frequently Asked Questions
What is the difference between CSA G40.21 300W and AS/NZS 1595 C350?
AS/NZS 1595 C350 specifies Si which is not specified for CSA G40.21 300W.
Can CSA G40.21 300W be substituted with AS/NZS 1595 C350?
CSA G40.21 300W and AS/NZS 1595 C350 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.