Minimal Match — 35% match
based on chemical composition and mechanical property overlap.
EN 10025-3 S460NL (EN 10025-3:2019) and ASTM A1008 SS Grade 50 (ASTM A1008) are both steel grades.
Both fall under the Structural Steel category.
EN 10025-3 S460NL is defined under European Standard (EN), originating from Europe, while ASTM A1008 SS Grade 50 is defined under ASTM International, originating from United States.
As per chemical composition, EN 10025-3 S460NL vs ASTM A1008 SS Grade 50 is a 61.4% match.
As per mechanical properties, the match is 0%.
Combined, this makes them a minimal match overall at 35%.
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property
EN 10025-3 S460NL
ASTM A1008 SS Grade 50
Tensile Strength
540-720 MPa
380 MPa min
Yield Strength
>=460 MPa
340 MPa min
Elongation
>=17%
14% min
Condition
Normalized or normalized rolled (N), nominal thickness up to 16 mm (tensile strength up to 100 mm), Table 4
EN 10025-3 S460NL specifies Nb, V, Ni, N which are not specified for ASTM A1008 SS Grade 50.
Can EN 10025-3 S460NL Be Substituted With ASTM A1008 SS Grade 50?
EN 10025-3 S460NL and ASTM A1008 SS Grade 50 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
What is the difference between EN 10025-3 S460NL and ASTM A1008 SS Grade 50?
EN 10025-3 S460NL specifies Nb, V, Ni, N which are not specified for ASTM A1008 SS Grade 50.
Can EN 10025-3 S460NL be substituted with ASTM A1008 SS Grade 50?
EN 10025-3 S460NL and ASTM A1008 SS Grade 50 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.