EN 10028-2 X12CrMo5 vs EN 10028-2 13CrMoSi5-5

Related Material — 69.9% match based on chemical composition and mechanical property overlap.

EN 10028-2 X12CrMo5 (EN 10028-2:2017) and EN 10028-2 13CrMoSi5-5 (EN 10028-2:2017) are both steel grades. Both fall under the Alloy Steel category. EN 10028-2 X12CrMo5 is typically used for flat products for pressure purposes, while EN 10028-2 13CrMoSi5-5 is commonly used for flat products for pressure purposes. EN 10028-2 X12CrMo5 is defined under European Standard (EN), originating from Europe, while EN 10028-2 13CrMoSi5-5 is defined under European Standard (EN), originating from Europe.

As per chemical composition, EN 10028-2 X12CrMo5 vs EN 10028-2 13CrMoSi5-5 is a 76.5% match. As per mechanical properties, the match is 66.7%. Combined, this makes them a related material overall at 69.9%.

Frequently Compared With EN 10028-2 X12CrMo5:
IS 1570 (Part 4) 10Cr20Mo6 IS 1570 (Part 4) 10Mo6 IS 1570 (Part 4) 07Cr4Mo6 IS 4367 07Cr4Mo6 NF A35-565 100C6 UNI 11234 100Cr6 IS 1570 (Part 4) 103Cr4 IS 1570 (Part 4) 103Cr6 IS 1570 (Part 4) 105Cr5 IS 1570 (Part 7) 10Cr36Mo10H IS 4367 10Cr9Mo10 EN 10028-2 10CrMo9-10
Match Breakdown
CHEMISTRY MATCH
76.5%
MECHANICAL MATCH
66.7%
OVERALL
69.9%
Specifications
Property EN 10028-2 X12CrMo5 EN 10028-2 13CrMoSi5-5
Standard EN 10028-2:2017 EN 10028-2:2017
Category Alloy Steel Alloy Steel
C (%) 0.10-0.15 <=0.17
Si (%) <=0.50 0.50-0.80
Mn (%) 0.30-0.60 0.40-0.65
P (%) <=0.020 <=0.015
S (%) <=0.005 <=0.005
N (%) <=0.012 <=0.012
Cr (%) 4.00-6.00 1.00-1.50
Cu (%) <=0.30 <=0.30
Mo (%) 0.45-0.65 0.45-0.65
Ni (%) <=0.30 <=0.30
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property EN 10028-2 X12CrMo5 EN 10028-2 13CrMoSi5-5
Tensile Strength 510-690 MPa 510-690 MPa
Yield Strength >=320 MPa >=310 MPa
Elongation >=20% >=20%
Condition Usual delivery condition normalized and tempered (+NT), nominal thickness up to 60 mm; transverse direction, Yield Strength is ReH, Elongation is A Usual delivery condition normalized and tempered (+NT), nominal thickness up to 60 mm; transverse direction, Yield Strength is ReH, Elongation is A
Typical Applications
EN 10028-2 X12CrMo5
Flat products for pressure purposes
EN 10028-2 13CrMoSi5-5
Flat products for pressure purposes
Can EN 10028-2 X12CrMo5 Be Substituted With EN 10028-2 13CrMoSi5-5?
EN 10028-2 X12CrMo5 and EN 10028-2 13CrMoSi5-5 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
On M-EX Right Now
EN 10028-2 X12CrMo5
0 active listings and RFQs →
EN 10028-2 13CrMoSi5-5
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10028-2 X12CrMo5 and EN 10028-2 13CrMoSi5-5?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can EN 10028-2 X12CrMo5 be substituted with EN 10028-2 13CrMoSi5-5?
EN 10028-2 X12CrMo5 and EN 10028-2 13CrMoSi5-5 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.