EN 10088-2 X50CrMoV15 vs EN 10088-1 X50CrMoV15

Strong Match — 93.1% match based on chemical composition and mechanical property overlap.

EN 10088-2 X50CrMoV15 (EN 10088-2:2014) and EN 10088-1 X50CrMoV15 (EN 10088-1:2023) are both steel grades. Both fall under the Stainless Steel category. EN 10088-2 X50CrMoV15 is defined under European Standard (EN), originating from Europe, while EN 10088-1 X50CrMoV15 is defined under European Standard (EN), originating from Europe.

As per chemical composition, EN 10088-2 X50CrMoV15 vs EN 10088-1 X50CrMoV15 is a 93.1% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a strong match overall at 93.1%.

Frequently Compared With EN 10088-2 X50CrMoV15:
ASTM A959 .- GB/T 3280 06Cr19Ni10 GOST 5632 06Kh23N28 GOST 5632 08X18H10 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12MoVH IS 1570 (Part 7) 12Cr12Ni2Mo EN 10088-1 1.4006 EN 10088-1 1.4301 EN 10088-1 1.4401 EN 10088-1 1.4845
Match Breakdown
CHEMISTRY MATCH
93.1%
MECHANICAL MATCH
No shared data
OVERALL
93.1%
Specifications
Property EN 10088-2 X50CrMoV15 EN 10088-1 X50CrMoV15
Standard EN 10088-2:2014 EN 10088-1:2023
Category Stainless Steel Stainless Steel
C (%) 0.45-0.55 0.35-0.55
Si (%) <=1.00 <=1.00
Mn (%) <=1.00 <=1.00
P (%) <=0.040 <=0.040
S (%) <=0.015 <=0.015
Cr (%) 14.0-15.0 14.0-15.5
Mo (%) 0.50-0.80 0.50-0.80
V (%) 0.10-0.20 0.10-0.20
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property EN 10088-2 X50CrMoV15 EN 10088-1 X50CrMoV15
Tensile Strength <=850 MPa Not specified
Elongation >=12% Not specified
Hardness <=280 HB Not specified
Condition Annealed (+A), cold rolled strip, up to 8 mm thick Not specified
Typical Applications
EN 10088-2 X50CrMoV15
General purposes, hot or cold rolled sheet/plate and strip
EN 10088-1 X50CrMoV15
Not documented
Can EN 10088-2 X50CrMoV15 Be Substituted With EN 10088-1 X50CrMoV15?
EN 10088-2 X50CrMoV15 and EN 10088-1 X50CrMoV15 overlap closely enough on chemistry and mechanical properties that EN 10088-1 X50CrMoV15 is often considered as a substitute for EN 10088-2 X50CrMoV15 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.
On M-EX Right Now
EN 10088-2 X50CrMoV15
0 active listings and RFQs →
EN 10088-1 X50CrMoV15
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10088-2 X50CrMoV15 and EN 10088-1 X50CrMoV15?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can EN 10088-2 X50CrMoV15 be substituted with EN 10088-1 X50CrMoV15?
EN 10088-2 X50CrMoV15 and EN 10088-1 X50CrMoV15 overlap closely enough on chemistry and mechanical properties that EN 10088-1 X50CrMoV15 is often considered as a substitute for EN 10088-2 X50CrMoV15 in many applications. Always confirm the specific property range your application needs before substituting, and check with your supplier's mill certificate.