Related Material — 65.7% match
based on chemical composition and mechanical property overlap.
EN 10346 S350GD (EN 10346:2015) and AS/NZS 3679.1 300 (AS/NZS 3679.1:2016) are both steel grades.
Both fall under the Structural Steel category.
EN 10346 S350GD is typically used for continuous hot-dip galvanized structural steel strip/sheet; roll-formed and cold-formed structural sections, purlins, roofing and cladding requiring corrosion protection, while AS/NZS 3679.1 300 is commonly used for hot-rolled structural bars and sections for general structural framing.
EN 10346 S350GD is defined under European Standard (EN), originating from Europe, while AS/NZS 3679.1 300 is defined under Australian/New Zealand Standard (AS/NZS), originating from Australia/New Zealand.
As per chemical composition, EN 10346 S350GD vs AS/NZS 3679.1 300 is a 98.5% match.
As per mechanical properties, the match is 0%.
Combined, this makes them a related material overall at 65.7%.
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property
EN 10346 S350GD
AS/NZS 3679.1 300
Tensile Strength
420 MPa min
440-600 MPa
Yield Strength
350 MPa min
300 MPa min
Elongation
14% min
22% min
Typical Applications
EN 10346 S350GD
Continuous hot-dip galvanized structural steel strip/sheet; roll-formed and cold-formed structural sections, purlins, roofing and cladding requiring corrosion protection
AS/NZS 3679.1 300
Hot-rolled structural bars and sections for general structural framing
Can EN 10346 S350GD Be Substituted With AS/NZS 3679.1 300?
EN 10346 S350GD and AS/NZS 3679.1 300 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
What is the difference between EN 10346 S350GD and AS/NZS 3679.1 300?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can EN 10346 S350GD be substituted with AS/NZS 3679.1 300?
EN 10346 S350GD and AS/NZS 3679.1 300 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.