GOST 14959 50HFA vs GB/T 3077 12Cr2Ni4A

Minimal Match — 35% match based on chemical composition and mechanical property overlap.

GOST 14959 50HFA (GOST 14959-2016) and GB/T 3077 12Cr2Ni4A (GB/T 3077-2015) are both steel grades. Both fall under the Alloy Steel category. GOST 14959 50HFA is typically used for used for coil springs, torsion bars, leaf springs, washers, and suspension parts., while GB/T 3077 12Cr2Ni4A is commonly used for used for gears, shafts, pinions, aircraft parts, heavy-duty bearings, and transmission components.. GB/T 3077 12Cr2Ni4A is defined under Guobiao Standards (GB/T) (China).

As per chemical composition, GOST 14959 50HFA vs GB/T 3077 12Cr2Ni4A is a 61.1% match. As per mechanical properties, the match is 0%. Combined, this makes them a minimal match overall at 35%.

Frequently Compared With GOST 14959 50HFA:
GOST 4543 12HN3A NF A35-565 100C6 UNI 11234 100Cr6 IS 4367 10Cr9Mo10 IS 4367 07Cr4Mo6 IS 1570 (Part 4) 103Cr4 IS 1570 (Part 4) 10Cr20Mo6 IS 1570 (Part 4) 103Cr6 IS 1570 (Part 4) 07Cr4Mo6 IS 1570 (Part 4) 105Cr5 IS 1570 (Part 7) 10Cr36Mo10H EN 10028-2 10CrMo9-10
Match Breakdown
CHEMISTRY MATCH
61.1%
MECHANICAL MATCH
0%
OVERALL
35%
Specifications
Property GOST 14959 50HFA GB/T 3077 12Cr2Ni4A
Standard GOST 14959-2016 GB/T 3077-2015
Category Alloy Steel Alloy Steel
C (%) 0.46-0.54 0.10-0.15
Cr (%) 0.8-1.1 1.25-1.65
V (%) 0.1-0.2 Not specified
Si (%) 0.17-0.37 0.17-0.37
Mn (%) 0.5-0.8 0.30-0.60
Ni (%) Not specified 3.25-3.75
P (%) Not specified 0.025 max
S (%) Not specified 0.025 max
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property GOST 14959 50HFA GB/T 3077 12Cr2Ni4A
Tensile Strength 1200-1500 MPa 980-1180 MPa
Yield Strength 1080 MPa min 785-980 MPa
Elongation 8% min 10-14%
Hardness 42-50 HRC 58-62 HRC (case)
Typical Applications
GOST 14959 50HFA
Used for coil springs, torsion bars, leaf springs, washers, and suspension parts.
GB/T 3077 12Cr2Ni4A
Used for gears, shafts, pinions, aircraft parts, heavy-duty bearings, and transmission components.
Key Differences
Can GOST 14959 50HFA Be Substituted With GB/T 3077 12Cr2Ni4A?
GOST 14959 50HFA and GB/T 3077 12Cr2Ni4A share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
Forms & Sizes Available on M-EX
GOST 14959 50HFA
Round Bar → (2 listings)
Diameter: 50–50 mm (1.97–1.97 in)
Length: 5500–6000 mm (216.54–236.22 in)
GB/T 3077 12Cr2Ni4A
Round Bar → (2 listings)
Diameter: 50–50 mm (1.97–1.97 in)
Length: 5000–6600 mm (196.85–259.84 in)
On M-EX Right Now
GOST 14959 50HFA
2 active listings and RFQs →
GB/T 3077 12Cr2Ni4A
2 active listings and RFQs →
Frequently Asked Questions
What is the difference between GOST 14959 50HFA and GB/T 3077 12Cr2Ni4A?
GOST 14959 50HFA specifies V which is not specified for GB/T 3077 12Cr2Ni4A. GB/T 3077 12Cr2Ni4A specifies Ni, P, S which are not specified for GOST 14959 50HFA.
Can GOST 14959 50HFA be substituted with GB/T 3077 12Cr2Ni4A?
GOST 14959 50HFA and GB/T 3077 12Cr2Ni4A share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.