JIS G4305:2012 SUS310S Steel: Specifications & Listings

JIS G4305:2012 SUS310S: SUS310S: austenitic stainless steel, cold-rolled plate, sheet and strip. Specified in JIS G 4305:2012.

Category: Stainless Steel
Grade Details
GradeJIS G4305:2012 SUS310S
Standard JIS G4305:2012
ApplicationsCold-rolled stainless steel plates, sheet and strip
Equivalent / Similar Grades
Grade Standard Region Live on M-EX
ASTM A959 310S ASTM A959:2011 USA No activity yet
ASTM A959 310Cb ASTM A959:2011 USA No activity yet
EN 10088-1 X8CrNi25-21 EN 10088-1:2023 Europe (CEN) No activity yet
JIS G4304 SUS310S JIS G4304:2021 Japan No activity yet
BS 970 (Part 3) 310S31 BS 970 (Part 3):1991 UK No activity yet
ASTM A959 SS310 ASTM A959:2011 USA 3 listings, 0 RFQs →
ASTM A959 310H ASTM A959:2011 USA No activity yet
Grade ComparisonCompare With a Specific Grade →
Grade Standard Match
JIS G4304 SUS310S JIS G4304:2021 Strong Match
ASTM A959 310S ASTM A959:2011 Strong Match
ASTM A959 310Cb ASTM A959:2011 Strong Match
BS 970 (Part 3) 310S31 BS 970 (Part 3):1991 Strong Match
BS 970 (Part 1) 310S31 BS 970 (Part 1):1983 Strong Match
ASTM A959 SS310 ASTM A959:2011 Strong Match
EN 10088-1 X8CrNi25-21 EN 10088-1:2014 Strong Match
EN 10088-1 X8CrNi25-21 EN 10088-1:2023 Strong Match
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Chemical Composition (%)
C Si Mn P S Ni Cr
<=0.08 <=1.50 <=2.00 <=0.045 <=0.030 19.00-22.00 24.00-26.00
Mechanical Properties
Tensile Strength >=520 MPa
Yield Strength >=205 MPa
Elongation >=40%
Hardness <=187 HB
Condition Solution heat treated plate and strip; 0.2 percent proof strength applies only when specified by the purchaser

More data from JIS G4305:2012

From the standard
Mechanical properties, solution heat treated 3 values
0.2 percent proof strength, min
205 MPa
Tensile strength, min
520 MPa
Elongation, min
40 %
0.2 percent proof strength applies only when specified by the purchaser. 1 N/mm2 = 1 MPa.
Source: JIS G 4305:2012, Table 8
Hardness, solution heat treated 3 scales
Brinell hardness HBW, max
187
Rockwell HRBW or HRBS, max
90
Vickers hardness HV, max
200
Any one of the hardness scales applies; if not specified the manufacturer selects. HRBW is used in case of dispute.
Source: JIS G 4305:2012, Table 8
Heat treatment (example, informative) 1 settings
Solution heat treatment
1030 to 1180 deg C, rapid cooling
Annex JA is informative; temperatures are examples.
Source: JIS G 4305:2012, Table JA.1

Active JIS G4305:2012 SUS310S Listings on M-EX (For Sale)

+ Create a Listing for this grade

No active JIS G4305:2012 SUS310S listings at this time.