SAE J403:2009 1018 Steel: Specifications & Listings

SAE J403:2009 1018: Nonresulfurized carbon steel SAE 1018 (UNS G10180) to SAE J403 DEC2009, a chemistry-only grade for semifinished products for forging, hot rolled and cold finished bars, wire rods, plates, strip, sheets, welded tubing and seamless tubing. Carbon 0.15-0.20% and manganese 0.60-0.90%.

Category: Carbon Steel
Grade Details
GradeSAE J403:2009 1018
Standard SAE J403:2009
ApplicationsChemistry-only grade; product scope as listed in the composition notes
Equivalent / Similar Grades
Grade Standard Region Live on M-EX
SAE J403 1018 SAE J403:2001 USA No activity yet
IS 1570 (Part 2/Sec 1) 15C8 IS 1570 (Part 2/Sec 1):1979 India No activity yet
IS 1570 (Part 2/Sec 1) 20C8 IS 1570 (Part 2/Sec 1):1979 India No activity yet
BS 970 (Part 1) 070M20 BS 970 (Part 1):1983 UK No activity yet
BS 970 (Part 1) 080A15 BS 970 (Part 1):1991 UK No activity yet
BS 970 (Part 1) 080M15 BS 970 (Part 1):1991 UK No activity yet
Grade ComparisonCompare With a Specific Grade →
Grade Standard Match
SAE J403 1018 SAE J403:2001 Strong Match
SAE J403 1018 SAE J403:2014 Strong Match
SAE J403 1019 SAE J403:2001 Strong Match
SAE J403 1019 SAE J403:2009 Strong Match
SAE J403 1019 SAE J403:2014 Strong Match
SAE J403 1016 SAE J403:2001 Strong Match
SAE J403 1016 SAE J403:2009 Strong Match
IS 1570 (Part 2/Sec 1) 15C8 IS 1570 (Part 2/Sec 1):1979 Strong Match
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Chemical Composition (%)
C Mn P S
0.15-0.20 0.60-0.90 <=0.030 <=0.050

More data from SAE J403:2009

From the standard
Other composition limits from the table and its notes
UNS number
G10180
Product scope
semifinished products for forging, hot rolled and cold finished bars, wire rods, plates, strip, sheets, welded tubing and seamless tubing
Residual limits, Option A
Cu 0.20, Ni 0.20, Cr 0.15, Mo 0.06 max
Residual limits, Option B (default)
Cu 0.35, Ni 0.25, Cr 0.20, Mo 0.06 max
Residual limits, Option C
Cu 0.40, Ni 0.40, Cr 0.30, Mo 0.12 max
Residual limits, Option D
No limits, values reported
Silicon, when required, is commonly specified as 0.10% max or a range such as 0.15 to 0.35%. Lead (0.15 to 0.35%, letter L) and boron (0.0005 to 0.003%, letter B) versions of the standard grades are identified by a letter between the second and third digits. Residual elements are agreed between purchaser and supplier; unless otherwise specified Option B applies. Option A applies to flat rolled products up to 1060.
Source: SAE J403:2009, Table 1, nonresulfurized carbon steels and its notes

Active SAE J403:2009 1018 Listings on M-EX (For Sale)

+ Create a Listing for this grade

No active SAE J403:2009 1018 listings at this time.

Register for Alerts

Buyer RFQs for SAE J403:2009 1018

+ Post an RFQ for this grade

No open buyer requirements for SAE J403:2009 1018 at this time.

Register for Alerts