ASTM A959:2011 316H Steel: Specifications & Listings

ASTM A959:2011 316H: Austenitic stainless steel type 316H (UNS S31609) with the composition limits of ASTM A959-11. Carbon 0.04-0.10% and chromium 16.0-18.0%.

Category: Stainless Steel
Grade Details
GradeASTM A959:2011 316H
Standard ASTM A959:2011
ApplicationsWrought stainless steel products; recommended composition limits for adoption by product standards (clause 1.1)
Equivalent / Similar Grades
Grade Standard Region Live on M-EX
IS 1570 (Part 7) 6Cr17Ni12Mo2H IS 1570 (Part 7):1992 India No activity yet
ASTM A240/A240M S31609 ASTM A240/A240M:2025 USA No activity yet
IS 1570 (Part 5) X04Cr17Ni12Mo2 IS 1570 (Part 5):1985 India No activity yet
IS 11169 (Part 2) X04Cr17Ni12Mo2Ti IS 11169 (Part 2):1989 India No activity yet
ASTM A276/A276M S31600 ASTM A276/A276M:2017 USA No activity yet
ASTM A240/A240M S31640 ASTM A240/A240M:2025 USA No activity yet
ASTM A240/A240M S31651 ASTM A240/A240M:2025 USA No activity yet
JIS G4304 SUS316 JIS G4304:2021 Japan No activity yet
JIS G4304 SUS316N JIS G4304:2021 Japan No activity yet
JIS G4304 SUS316Ti JIS G4304:2021 Japan No activity yet
Grade ComparisonCompare With a Specific Grade →
Grade Standard Match
ASTM A240/A240M S31609 ASTM A240/A240M:2025 Strong Match
ASTM A959 SS316 ASTM A959:2011 Strong Match
IS 1570 (Part 5) X04Cr17Ni12Mo2 IS 1570 (Part 5):1985 Strong Match
IS 1570 (Part 7) 6Cr17Ni12Mo2H IS 1570 (Part 7):1992 Strong Match
IS 11169 (Part 2) X04Cr17Ni12Mo2 IS 11169 (Part 2):1989 Strong Match
IS 11169 (Part 2) X04Cr17Ni12Mo2Ti IS 11169 (Part 2):1989 Strong Match
IS 6911 X04Cr17Ni12Mo2 IS 6911:1992 Strong Match
IS 6911 X04Cr17Ni12Mo2Ti IS 6911:1992 Strong Match
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Chemical Composition (%)
C Cr Mn Mo Ni P S Si
0.04-0.10 16.0-18.0 <=2.00 2.00-3.00 10.0-14.0 <=0.045 <=0.030 <=1.00

More data from ASTM A959:2011

From the standard
Other composition limits from Table 1 and its footnotes
UNS number
S31609
Metallurgical class
Austenitic grade: usually predominantly face-centered cubic, hardenable only by cold working
Type
316H (common type number, not a trademark, widely used; not associated with any one product)
Values
Maximum unless a range or minimum is shown; where two limits are shown for the same element in one grade the more stringent applies
These are the recommended composition limits of the A959 guide, intended for adoption by standards for stainless steel products; they are not a product specification.
Source: ASTM A959:2011, Table 1 and its footnotes

Active ASTM A959:2011 316H Listings on M-EX (For Sale)

+ Create a Listing for this grade

No active ASTM A959:2011 316H listings at this time.