ASTM A959:2011 S40975 Steel: Specifications & Listings

ASTM A959:2011 S40975: Ferritic stainless steel grade (UNS S40975) with the composition limits of ASTM A959-11. Carbon up to 0.030% and chromium 10.5-11.7%.

Category: Stainless Steel
Grade Details
GradeASTM A959:2011 S40975
Standard ASTM A959:2011
ApplicationsWrought stainless steel products; recommended composition limits for adoption by product standards (clause 1.1)
Equivalent / Similar Grades
Grade Standard Region Live on M-EX
ASTM A959 S40945 ASTM A959:2011 USA No activity yet
ASTM A240/A240M S40975 ASTM A240/A240M:2025 USA No activity yet
EN 10088-3 X2CrNi12 EN 10088-3:2014 Europe No activity yet
ASTM A240/A240M S40977 ASTM A240/A240M:2025 USA No activity yet
EN 10088-1 X2CrNi12 EN 10088-1:2014 Europe (CEN) No activity yet
ASTM A240/A240M S41003 ASTM A240/A240M:2025 USA No activity yet
ASTM A276/A276M S40976 ASTM A276/A276M:2017 USA No activity yet
ASTM A240/A240M S41050 ASTM A240/A240M:2025 USA No activity yet
ASTM A240/A240M S40930 ASTM A240/A240M:2025 USA No activity yet
Grade ComparisonCompare With a Specific Grade →
Grade Standard Match
ASTM A240/A240M S40975 ASTM A240/A240M:2025 Strong Match
EN 10088-3 X2CrNi12 EN 10088-3:2014 Strong Match
ASTM A959 S40977 ASTM A959:2011 Strong Match
ASTM A240/A240M S40977 ASTM A240/A240M:2025 Strong Match
EN 10088-1 X2CrNi12 EN 10088-1:2014 Strong Match
EN 10088-2 X2CrNi12 EN 10088-2:2014 Strong Match
ASTM A959 S40910 ASTM A959:2011 Strong Match
ASTM A959 S40920 ASTM A959:2011 Strong Match
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Chemical Composition (%)
C Cr Mn N Ni P S Si
<=0.030 10.5-11.7 <=1.00 <=0.030 0.50-1.00 <=0.040 <=0.030 <=1.00

More data from ASTM A959:2011

From the standard
Other composition limits from Table 1 and its footnotes
UNS number
S40975
Metallurgical class
Ferritic grade: body-centered cubic, little or no tempered martensite, hardenable only slightly by cold working
Type
No type number is printed; the grade is identified by its UNS number only
Values
Maximum unless a range or minimum is shown; where two limits are shown for the same element in one grade the more stringent applies
Other elements (as printed)
Ti 6(C+N) min; 0.75 max
These are the recommended composition limits of the A959 guide, intended for adoption by standards for stainless steel products; they are not a product specification.
Source: ASTM A959:2011, Table 1 and its footnotes

Active ASTM A959:2011 S40975 Listings on M-EX (For Sale)

+ Create a Listing for this grade

No active ASTM A959:2011 S40975 listings at this time.

Register for Alerts

Buyer RFQs for ASTM A959:2011 S40975

+ Post an RFQ for this grade

No open buyer requirements for ASTM A959:2011 S40975 at this time.

Register for Alerts