CSA G40.21 350W vs ASTM A1008 SS Grade 80

Related Material — 62.4% match based on chemical composition and mechanical property overlap.

CSA G40.21 350W (CSA G40.21-13 (R2023)) and ASTM A1008 SS Grade 80 (ASTM A1008) are both steel grades. Both fall under the Structural Steel category. CSA G40.21 350W is typically used for used in buildings, bridges, cranes, transmission towers, heavy equipment, and structural fabrications., while ASTM A1008 SS Grade 80 is commonly used for cold-rolled high-strength structural steel sheet, higher strength grade; automotive structural/reinforcement components, cold-formed high-strength parts. CSA G40.21 350W is defined under Canadian Standards Association (CSA), originating from Canada, while ASTM A1008 SS Grade 80 is defined under ASTM International, originating from United States.

As per chemical composition, CSA G40.21 350W vs ASTM A1008 SS Grade 80 is a 93.6% match. As per mechanical properties, the match is 0%. Combined, this makes them a related material overall at 62.4%.

Frequently Compared With CSA G40.21 350W:
AS/NZS 3679.1 350 IS 2062 E250B0 CSA G40.21 480W AS/NZS 1595 C350 AS/NZS 1595 C450 CSA G40.21 400A CSA G40.21 260W IS 2062 E250A CSA G40.21 400W GOST 19281 09G2S ASTM A572 Gr.65 ASTM A572 Grade 50
Match Breakdown
CHEMISTRY MATCH
93.6%
MECHANICAL MATCH
0%
OVERALL
62.4%
Specifications
Property CSA G40.21 350W ASTM A1008 SS Grade 80
Standard CSA G40.21-13 (R2023) ASTM A1008
Category Structural Steel Structural Steel
C (%) 0.23 max <=0.25
Mn (%) 0.50-1.50 <=1.65
Si (%) 0.15-0.40 <=0.50
P (%) 0.040 max <=0.040
S (%) 0.050 max <=0.040
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property CSA G40.21 350W ASTM A1008 SS Grade 80
Tensile Strength 450-620 MPa 570 MPa min
Yield Strength 350 MPa min 550 MPa min
Elongation 20% min 10% min
Hardness 135-180 HB Not specified
Typical Applications
CSA G40.21 350W
Used in buildings, bridges, cranes, transmission towers, heavy equipment, and structural fabrications.
ASTM A1008 SS Grade 80
Cold-rolled high-strength structural steel sheet, higher strength grade; automotive structural/reinforcement components, cold-formed high-strength parts
Can CSA G40.21 350W Be Substituted With ASTM A1008 SS Grade 80?
CSA G40.21 350W and ASTM A1008 SS Grade 80 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
Forms & Sizes Available on M-EX
CSA G40.21 350W
Plate → (2 listings)
Thickness: 10–10 mm (0.39–0.39 in)
Width: 1500–1500 mm (59.06–59.06 in)
Length: 2700–3400 mm (106.3–133.86 in)
ASTM A1008 SS Grade 80
Plate → (2 listings)
Thickness: 10–10 mm (0.39–0.39 in)
Width: 1500–1500 mm (59.06–59.06 in)
Length: 2500–3700 mm (98.43–145.67 in)
On M-EX Right Now
CSA G40.21 350W
2 active listings and RFQs →
ASTM A1008 SS Grade 80
2 active listings and RFQs →
Frequently Asked Questions
What is the difference between CSA G40.21 350W and ASTM A1008 SS Grade 80?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can CSA G40.21 350W be substituted with ASTM A1008 SS Grade 80?
CSA G40.21 350W and ASTM A1008 SS Grade 80 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.