Close Alternative — 70.9% match
based on chemical composition and mechanical property overlap.
EN 10025-3 S500 (EN 10025-3:2019) and ASTM A572/A572M Grade 60 (ASTM A572/A572M:2021) are both steel grades.
Both fall under the Structural Steel category.
EN 10025-3 S500 is typically used for used in heavy structural sections, mining equipment, bridge fabrication, transport vehicles, and offshore structures., while ASTM A572/A572M Grade 60 is commonly used for riveted or bolted bridge construction, or riveted, bolted or welded construction in other applications.
EN 10025-3 S500 is defined under European Standard (EN), originating from Europe, while ASTM A572/A572M Grade 60 is defined under ASTM International, originating from United States.
As per chemical composition, EN 10025-3 S500 vs ASTM A572/A572M Grade 60 is a 89.6% match.
As per mechanical properties, the match is 33.3%.
Combined, this makes them a close alternative overall at 70.9%.
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property
EN 10025-3 S500
ASTM A572/A572M Grade 60
Tensile Strength
590-770 MPa
>=520 MPa
Yield Strength
500 MPa min
>=415 MPa
Elongation
16% min
>=16%
Hardness
190-240 HB
Not specified
Condition
Not specified
Tension test per Table 4; one set of minimum values for all product thicknesses; Elongation is in 200 mm gauge length, 50 mm values in the tensile block
Typical Applications
EN 10025-3 S500
Used in heavy structural sections, mining equipment, bridge fabrication, transport vehicles, and offshore structures.
ASTM A572/A572M Grade 60
Riveted or bolted bridge construction, or riveted, bolted or welded construction in other applications
Key Differences
EN 10025-3 S500 specifies Nb, V, Ti which are not specified for ASTM A572/A572M Grade 60.
Can EN 10025-3 S500 Be Substituted With ASTM A572/A572M Grade 60?
EN 10025-3 S500 and ASTM A572/A572M Grade 60 are a close alternative rather than a direct substitute. Some properties overlap well, but check the specific chemistry and mechanical rows above against your application's requirements before treating them as interchangeable.
What is the difference between EN 10025-3 S500 and ASTM A572/A572M Grade 60?
EN 10025-3 S500 specifies Nb, V, Ti which are not specified for ASTM A572/A572M Grade 60.
Can EN 10025-3 S500 be substituted with ASTM A572/A572M Grade 60?
EN 10025-3 S500 and ASTM A572/A572M Grade 60 are a close alternative rather than a direct substitute. Some properties overlap well, but check the specific chemistry and mechanical rows above against your application's requirements before treating them as interchangeable.