Related Material — 69.9% match
based on chemical composition and mechanical property overlap.
JIS G4053 SMnC420 (JIS G4053:2008) and IS 1570 (Part 4) 103Cr6 (IS 1570 (Part 4):1988) are both steel grades.
Both fall under the Alloy Steel category.
JIS G4053 SMnC420 is defined under Japanese Industrial Standards (JIS), originating from Japan, while IS 1570 (Part 4) 103Cr6 is defined under Bureau of Indian Standards (IS), originating from India.
As per chemical composition, JIS G4053 SMnC420 vs IS 1570 (Part 4) 103Cr6 is a 76% match.
Mechanical property data is not available for both grades, so this factor could not be scored.
Combined, this makes them a related material overall at 69.9%.
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property
JIS G4053 SMnC420
IS 1570 (Part 4) 103Cr6
Tensile Strength
785–980 MPa
Not specified
Case Hardness HRC
58–62
Not specified
Core Hardness HB
217–277
Not specified
Elongation
≥10%
Not specified
Typical Applications
JIS G4053 SMnC420
Case hardened gears, shafts, cams, pins, automotive components
IS 1570 (Part 4) 103Cr6
Not documented
Key Differences
JIS G4053 SMnC420 specifies S, P which are not specified for IS 1570 (Part 4) 103Cr6.
Can JIS G4053 SMnC420 Be Substituted With IS 1570 (Part 4) 103Cr6?
JIS G4053 SMnC420 and IS 1570 (Part 4) 103Cr6 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
What is the difference between JIS G4053 SMnC420 and IS 1570 (Part 4) 103Cr6?
JIS G4053 SMnC420 specifies S, P which are not specified for IS 1570 (Part 4) 103Cr6.
Can JIS G4053 SMnC420 be substituted with IS 1570 (Part 4) 103Cr6?
JIS G4053 SMnC420 and IS 1570 (Part 4) 103Cr6 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.