Related Material — 61% match
based on chemical composition and mechanical property overlap.
EN 10025-2 E360 (EN 10025-2:2019) and ASTM A36 (ASTM A36) are both steel grades.
EN 10025-2 E360 is classified under Structural Steel, while ASTM A36 is classified under Carbon Steel — a different category, which is worth noting alongside the chemistry match below.
EN 10025-2 E360 is typically used for hot rolled products of structural steels, while ASTM A36 is commonly used for structural fabrication, bridges, buildings, machinery parts, flanges.
EN 10025-2 E360 is defined under European Standard (EN), originating from Europe, while ASTM A36 is defined under ASTM International, originating from United States.
As per chemical composition, EN 10025-2 E360 vs ASTM A36 is a 91.5% match.
As per mechanical properties, the match is 0%.
Combined, this makes them a related material overall at 61%.
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property
EN 10025-2 E360
ASTM A36
Tensile Strength
670-830 MPa
400–550 MPa
Yield Strength
>=360 MPa
250 MPa min
Elongation
>=11%
≥23%
Condition
Nominal thickness up to 16 mm (tensile for 3 to 100 mm, elongation for 3 to 40 mm), longitudinal test pieces
Different category: EN 10025-2 E360 is Structural Steel, ASTM A36 is Carbon Steel.
EN 10025-2 E360 specifies N which is not specified for ASTM A36.
ASTM A36 specifies C, Mn, Si which are not specified for EN 10025-2 E360.
Can EN 10025-2 E360 Be Substituted With ASTM A36?
EN 10025-2 E360 and ASTM A36 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
What is the difference between EN 10025-2 E360 and ASTM A36?
Different category: EN 10025-2 E360 is Structural Steel, ASTM A36 is Carbon Steel. EN 10025-2 E360 specifies N which is not specified for ASTM A36. ASTM A36 specifies C, Mn, Si which are not specified for EN 10025-2 E360.
Can EN 10025-2 E360 be substituted with ASTM A36?