EN 10088-1 1.4845 vs EN 10088-1 1.4006

Minimal Match — 35% match based on chemical composition and mechanical property overlap.

EN 10088-1 1.4845 (EN 10088-1:2014) and EN 10088-1 1.4006 (EN 10088-1:2014) are both steel grades. Both fall under the Stainless Steel category. EN 10088-1 1.4845 is typically used for furnace parts, heat exchangers, kiln components, while EN 10088-1 1.4006 is commonly used for cutlery, turbine blades, fasteners, surgical instruments. EN 10088-1 1.4845 is defined under European Standard (EN), originating from Europe, while EN 10088-1 1.4006 is defined under European Standard (EN), originating from Europe.

As per chemical composition, EN 10088-1 1.4845 vs EN 10088-1 1.4006 is a 75% match. As per mechanical properties, the match is 0%. Combined, this makes them a minimal match overall at 35%.

Frequently Compared With EN 10088-1 1.4845:
EN 10088-1 1.4401 EN 10088-1 1.4301 GOST 5632 06Kh23N28 GB/T 3280 06Cr19Ni10 GOST 5632 08X18H10 GOST 5632 12Kh13 ASTM A959 202 ASTM A959 16-8-2H IS 1570 (Part 7) 12Cr13H ASTM A959 301 ASTM A959 201 ASTM A959 26-3-3
Match Breakdown
CHEMISTRY MATCH
75%
MECHANICAL MATCH
0%
OVERALL
35%
Specifications
Property EN 10088-1 1.4845 EN 10088-1 1.4006
Standard EN 10088-1:2014 EN 10088-1:2014
Category Stainless Steel Stainless Steel
C (%) ≤0.10 0.08–0.15
Si (%) ≤1.50 ≤1.00
Mn (%) ≤2.00 ≤1.50
Cr (%) 24.0–26.0 11.5–13.5
Ni (%) 19.0–22.0 ≤0.75
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property EN 10088-1 1.4845 EN 10088-1 1.4006
Tensile Strength ≥515 MPa ≥540 MPa (annealed)
Yield Strength ≥205 MPa Not specified
Elongation ≥40% ≥18%
Max Service Temp 1100°C continuous Not specified
Hardness HRC Not specified 36–45 (hardened)
Typical Applications
EN 10088-1 1.4845
Furnace parts, heat exchangers, kiln components
EN 10088-1 1.4006
Cutlery, turbine blades, fasteners, surgical instruments
Can EN 10088-1 1.4845 Be Substituted With EN 10088-1 1.4006?
EN 10088-1 1.4845 and EN 10088-1 1.4006 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
Forms & Sizes Available on M-EX
EN 10088-1 1.4845
Sheet → (3 listings)
Thickness: 6–6 mm (0.24–0.24 in)
Width: 1250–1250 mm (49.21–49.21 in)
Length: 2700–3200 mm (106.3–125.98 in)
EN 10088-1 1.4006
Sheet → (3 listings)
Thickness: 6–6 mm (0.24–0.24 in)
Width: 1250–1250 mm (49.21–49.21 in)
Length: 2700–3400 mm (106.3–133.86 in)
On M-EX Right Now
EN 10088-1 1.4845
3 active listings and RFQs →
EN 10088-1 1.4006
3 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10088-1 1.4845 and EN 10088-1 1.4006?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can EN 10088-1 1.4845 be substituted with EN 10088-1 1.4006?
EN 10088-1 1.4845 and EN 10088-1 1.4006 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.