GOST 5632 08X18H10 vs EN 10088-1 1.4301

Close Alternative — 72.8% match based on chemical composition and mechanical property overlap.

GOST 5632 08X18H10 (GOST 5632-2014) and EN 10088-1 1.4301 (EN 10088-1:2014) are both steel grades. Both fall under the Stainless Steel category. GOST 5632 08X18H10 is typically used for chemical equipment, food processing, general corrosion resistant applications, while EN 10088-1 1.4301 is commonly used for food equipment, chemical vessels, architectural, kitchenware. EN 10088-1 1.4301 is defined under European Standard (EN) (Europe).

As per chemical composition, GOST 5632 08X18H10 vs EN 10088-1 1.4301 is a 92.5% match. As per mechanical properties, the match is 33.3%. Combined, this makes them a close alternative overall at 72.8%.

Frequently Compared With GOST 5632 08X18H10:
EN 10088-1 1.4845 EN 10088-1 1.4006 EN 10088-1 1.4401 ASTM A959 201 ASTM A959 .- ASTM A959 16-8-2H ASTM A959 202 ASTM A959 26-3-3 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 20Cr12MoNiVH IS 1570 (Part 7) 12Cr12Ni2Mo IS 1570 (Part 7) 12Cr13H
Match Breakdown
CHEMISTRY MATCH
92.5%
MECHANICAL MATCH
33.3%
OVERALL
72.8%
Specifications
Property GOST 5632 08X18H10 EN 10088-1 1.4301
Standard GOST 5632-2014 EN 10088-1:2014
Category Stainless Steel Stainless Steel
C (%) ≤0.08 ≤0.07
Si (%) ≤0.80 ≤1.00
Mn (%) ≤2.00 ≤2.00
Cr (%) 17.0–19.0 17.5–19.5
Ni (%) 9.0–11.0 8.0–10.5
S (%) ≤0.020 ≤0.030
P (%) ≤0.035 ≤0.045
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property GOST 5632 08X18H10 EN 10088-1 1.4301
Tensile Strength ≥520 MPa ≥520 MPa
Yield Strength ≥205 MPa ≥210 MPa
Elongation ≥40% ≥45%
Hardness Not specified ≤215 HB
Typical Applications
GOST 5632 08X18H10
Chemical equipment, food processing, general corrosion resistant applications
EN 10088-1 1.4301
Food equipment, chemical vessels, architectural, kitchenware
Can GOST 5632 08X18H10 Be Substituted With EN 10088-1 1.4301?
GOST 5632 08X18H10 and EN 10088-1 1.4301 are a close alternative rather than a direct substitute. Some properties overlap well, but check the specific chemistry and mechanical rows above against your application's requirements before treating them as interchangeable.
Forms & Sizes Available on M-EX
GOST 5632 08X18H10
Sheet → (2 listings)
Thickness: 6–6 mm (0.24–0.24 in)
Width: 1250–1250 mm (49.21–49.21 in)
Length: 2500–2700 mm (98.43–106.3 in)
EN 10088-1 1.4301
Sheet → (3 listings)
Thickness: 6–6 mm (0.24–0.24 in)
Width: 1250–1250 mm (49.21–49.21 in)
Length: 2500–3300 mm (98.43–129.92 in)
On M-EX Right Now
GOST 5632 08X18H10
2 active listings and RFQs →
EN 10088-1 1.4301
3 active listings and RFQs →
Frequently Asked Questions
What is the difference between GOST 5632 08X18H10 and EN 10088-1 1.4301?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can GOST 5632 08X18H10 be substituted with EN 10088-1 1.4301?
GOST 5632 08X18H10 and EN 10088-1 1.4301 are a close alternative rather than a direct substitute. Some properties overlap well, but check the specific chemistry and mechanical rows above against your application's requirements before treating them as interchangeable.