GOST 5632 08X18H10 vs EN 10088-1 1.4845

Related Material — 69.9% match based on chemical composition and mechanical property overlap.

GOST 5632 08X18H10 (GOST 5632-2014) and EN 10088-1 1.4845 (EN 10088-1:2014) are both steel grades. Both fall under the Stainless Steel category. GOST 5632 08X18H10 is typically used for chemical equipment, food processing, general corrosion resistant applications, while EN 10088-1 1.4845 is commonly used for furnace parts, heat exchangers, kiln components. EN 10088-1 1.4845 is defined under European Standard (EN) (Europe).

As per chemical composition, GOST 5632 08X18H10 vs EN 10088-1 1.4845 is a 83.3% match. As per mechanical properties, the match is 66.7%. Combined, this makes them a related material overall at 69.9%.

Frequently Compared With GOST 5632 08X18H10:
EN 10088-1 1.4301 EN 10088-1 1.4006 EN 10088-1 1.4401 ASTM A959 201 ASTM A959 .- ASTM A959 16-8-2H ASTM A959 202 ASTM A959 26-3-3 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 20Cr12MoNiVH IS 1570 (Part 7) 12Cr12Ni2Mo IS 1570 (Part 7) 12Cr13H
Match Breakdown
CHEMISTRY MATCH
83.3%
MECHANICAL MATCH
66.7%
OVERALL
69.9%
Specifications
Property GOST 5632 08X18H10 EN 10088-1 1.4845
Standard GOST 5632-2014 EN 10088-1:2014
Category Stainless Steel Stainless Steel
C (%) ≤0.08 ≤0.10
Si (%) ≤0.80 ≤1.50
Mn (%) ≤2.00 ≤2.00
Cr (%) 17.0–19.0 24.0–26.0
Ni (%) 9.0–11.0 19.0–22.0
S (%) ≤0.020 Not specified
P (%) ≤0.035 Not specified
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property GOST 5632 08X18H10 EN 10088-1 1.4845
Tensile Strength ≥520 MPa ≥515 MPa
Yield Strength ≥205 MPa ≥205 MPa
Elongation ≥40% ≥40%
Max Service Temp Not specified 1100°C continuous
Typical Applications
GOST 5632 08X18H10
Chemical equipment, food processing, general corrosion resistant applications
EN 10088-1 1.4845
Furnace parts, heat exchangers, kiln components
Key Differences
Can GOST 5632 08X18H10 Be Substituted With EN 10088-1 1.4845?
GOST 5632 08X18H10 and EN 10088-1 1.4845 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
Forms & Sizes Available on M-EX
GOST 5632 08X18H10
Sheet → (2 listings)
Thickness: 6–6 mm (0.24–0.24 in)
Width: 1250–1250 mm (49.21–49.21 in)
Length: 2500–2700 mm (98.43–106.3 in)
EN 10088-1 1.4845
Sheet → (3 listings)
Thickness: 6–6 mm (0.24–0.24 in)
Width: 1250–1250 mm (49.21–49.21 in)
Length: 2700–3200 mm (106.3–125.98 in)
On M-EX Right Now
GOST 5632 08X18H10
2 active listings and RFQs →
EN 10088-1 1.4845
3 active listings and RFQs →
Frequently Asked Questions
What is the difference between GOST 5632 08X18H10 and EN 10088-1 1.4845?
GOST 5632 08X18H10 specifies S, P which are not specified for EN 10088-1 1.4845.
Can GOST 5632 08X18H10 be substituted with EN 10088-1 1.4845?
GOST 5632 08X18H10 and EN 10088-1 1.4845 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.