NF A35-574 Z7CN18-09 vs EN 10088-1 1.4301

Minimal Match — 35% match based on chemical composition and mechanical property overlap.

NF A35-574 Z7CN18-09 (NF A35-574:1990) and EN 10088-1 1.4301 (EN 10088-1:2014) are both steel grades. Both fall under the Stainless Steel category. NF A35-574 Z7CN18-09 is typically used for used for food processing equipment, kitchen equipment, chemical tanks, piping, architectural components, and fasteners., while EN 10088-1 1.4301 is commonly used for food equipment, chemical vessels, architectural, kitchenware. NF A35-574 Z7CN18-09 is defined under Association Francaise de Normalisation (NF), originating from France, while EN 10088-1 1.4301 is defined under European Standard (EN), originating from Europe.

As per chemical composition, NF A35-574 Z7CN18-09 vs EN 10088-1 1.4301 is a 81.5% match. As per mechanical properties, the match is 0%. Combined, this makes them a minimal match overall at 35%.

Frequently Compared With NF A35-574 Z7CN18-09:
GB/T 3280 06Cr19Ni10 GOST 5632 12Kh13 GOST 5632 06Kh23N28 EN 10088-1 1.4845 GOST 5632 08X18H10 EN 10088-1 1.4401 EN 10088-1 1.4006 ASTM A959 .- IS 1570 (Part 7) 12Cr12MoH IS 1570 (Part 7) 12Cr12MoVH IS 1570 (Part 7) 12Cr12Ni2Mo IS 1570 (Part 7) 11Cr17Ni13W3TiH
Match Breakdown
CHEMISTRY MATCH
81.5%
MECHANICAL MATCH
0%
OVERALL
35%
Specifications
Property NF A35-574 Z7CN18-09 EN 10088-1 1.4301
Standard NF A35-574:1990 EN 10088-1:2014
Category Stainless Steel Stainless Steel
C (%) 0.08 max ≤0.07
Si (%) 1.00 max ≤1.00
Mn (%) 2.00 max ≤2.00
Cr (%) 17.00-19.00 17.5–19.5
Ni (%) 8.00-10.50 8.0–10.5
P (%) 0.045 max ≤0.045
S (%) 0.030 max ≤0.030
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property NF A35-574 Z7CN18-09 EN 10088-1 1.4301
Tensile Strength 500-700 MPa ≥520 MPa
Yield Strength 190-250 MPa ≥210 MPa
Elongation 40-55% ≥45%
Hardness 140-210 HB ≤215 HB
Typical Applications
NF A35-574 Z7CN18-09
Used for food processing equipment, kitchen equipment, chemical tanks, piping, architectural components, and fasteners.
EN 10088-1 1.4301
Food equipment, chemical vessels, architectural, kitchenware
Can NF A35-574 Z7CN18-09 Be Substituted With EN 10088-1 1.4301?
NF A35-574 Z7CN18-09 and EN 10088-1 1.4301 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
Forms & Sizes Available on M-EX
NF A35-574 Z7CN18-09
Sheet → (2 listings)
Thickness: 6–6 mm (0.24–0.24 in)
Width: 1250–1250 mm (49.21–49.21 in)
Length: 2600–2900 mm (102.36–114.17 in)
EN 10088-1 1.4301
Sheet → (3 listings)
Thickness: 6–6 mm (0.24–0.24 in)
Width: 1250–1250 mm (49.21–49.21 in)
Length: 2500–3300 mm (98.43–129.92 in)
On M-EX Right Now
NF A35-574 Z7CN18-09
2 active listings and RFQs →
EN 10088-1 1.4301
3 active listings and RFQs →
Frequently Asked Questions
What is the difference between NF A35-574 Z7CN18-09 and EN 10088-1 1.4301?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can NF A35-574 Z7CN18-09 be substituted with EN 10088-1 1.4301?
NF A35-574 Z7CN18-09 and EN 10088-1 1.4301 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.