EN 10088-1 1.4006 vs EN 10088-1 1.4845

Minimal Match — 35% match based on chemical composition and mechanical property overlap.

EN 10088-1 1.4006 (EN 10088-1:2014) and EN 10088-1 1.4845 (EN 10088-1:2014) are both steel grades. Both fall under the Stainless Steel category. EN 10088-1 1.4006 is typically used for cutlery, turbine blades, fasteners, surgical instruments, while EN 10088-1 1.4845 is commonly used for furnace parts, heat exchangers, kiln components. EN 10088-1 1.4006 is defined under European Standard (EN), originating from Europe, while EN 10088-1 1.4845 is defined under European Standard (EN), originating from Europe.

As per chemical composition, EN 10088-1 1.4006 vs EN 10088-1 1.4845 is a 75% match. As per mechanical properties, the match is 0%. Combined, this makes them a minimal match overall at 35%.

Frequently Compared With EN 10088-1 1.4006:
GB/T 3280 06Cr19Ni10 GOST 5632 12Kh13 GOST 5632 08X18H10 GOST 5632 06Kh23N28 EN 10088-1 1.4301 EN 10088-1 1.4401 ASTM A959 2205 IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr13H ASTM A959 202 IS 1570 (Part 7) 12Cr12MoVH IS 1570 (Part 7) 12Cr12Ni2Mo
Match Breakdown
CHEMISTRY MATCH
75%
MECHANICAL MATCH
0%
OVERALL
35%
Specifications
Property EN 10088-1 1.4006 EN 10088-1 1.4845
Standard EN 10088-1:2014 EN 10088-1:2014
Category Stainless Steel Stainless Steel
C (%) 0.08–0.15 ≤0.10
Si (%) ≤1.00 ≤1.50
Mn (%) ≤1.50 ≤2.00
Cr (%) 11.5–13.5 24.0–26.0
Ni (%) ≤0.75 19.0–22.0
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property EN 10088-1 1.4006 EN 10088-1 1.4845
Tensile Strength ≥540 MPa (annealed) ≥515 MPa
Hardness HRC 36–45 (hardened) Not specified
Elongation ≥18% ≥40%
Yield Strength Not specified ≥205 MPa
Max Service Temp Not specified 1100°C continuous
Typical Applications
EN 10088-1 1.4006
Cutlery, turbine blades, fasteners, surgical instruments
EN 10088-1 1.4845
Furnace parts, heat exchangers, kiln components
Can EN 10088-1 1.4006 Be Substituted With EN 10088-1 1.4845?
EN 10088-1 1.4006 and EN 10088-1 1.4845 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
Forms & Sizes Available on M-EX
EN 10088-1 1.4006
Sheet → (3 listings)
Thickness: 6–6 mm (0.24–0.24 in)
Width: 1250–1250 mm (49.21–49.21 in)
Length: 2700–3400 mm (106.3–133.86 in)
EN 10088-1 1.4845
Sheet → (3 listings)
Thickness: 6–6 mm (0.24–0.24 in)
Width: 1250–1250 mm (49.21–49.21 in)
Length: 2700–3200 mm (106.3–125.98 in)
On M-EX Right Now
EN 10088-1 1.4006
3 active listings and RFQs →
EN 10088-1 1.4845
3 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10088-1 1.4006 and EN 10088-1 1.4845?
Both grades share a similar composition profile; see the specification table above for the exact chemistry and mechanical property values.
Can EN 10088-1 1.4006 be substituted with EN 10088-1 1.4845?
EN 10088-1 1.4006 and EN 10088-1 1.4845 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.