EN 10088-1 1.4301 vs ASTM A959 .-

Related Material — 65% match based on chemical composition and mechanical property overlap.

EN 10088-1 1.4301 (EN 10088-1:2014) and ASTM A959 .- (ASTM A959:2011) are both steel grades. Both fall under the Stainless Steel category. EN 10088-1 1.4301 is typically used for food equipment, chemical vessels, architectural, kitchenware, while ASTM A959 .- is commonly used for wrought stainless steel products; recommended composition limits for adoption by product standards (clause 1.1). EN 10088-1 1.4301 is defined under European Standard (EN), originating from Europe, while ASTM A959 .- is defined under ASTM International, originating from United States.

As per chemical composition, EN 10088-1 1.4301 vs ASTM A959 .- is a 65% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a related material overall at 65%.

Frequently Compared With EN 10088-1 1.4301:
EN 10088-1 1.4401 EN 10088-1 1.4845 GOST 5632 06Kh23N28 GOST 5632 08X18H10 GB/T 3280 06Cr19Ni10 GOST 5632 12Kh13 EN 10088-1 1.4006 IS 1570 (Part 7) 12Cr13H IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoVH ASTM A959 202 IS 1570 (Part 7) 20Cr12MoNiVH
Match Breakdown
CHEMISTRY MATCH
65%
MECHANICAL MATCH
No shared data
OVERALL
65%
Specifications
Property EN 10088-1 1.4301 ASTM A959 .-
Standard EN 10088-1:2014 ASTM A959:2011
Category Stainless Steel Stainless Steel
C (%) ≤0.07 <=0.030
Si (%) ≤1.00 <=1.00
Mn (%) ≤2.00 <=1.00
Cr (%) 17.5–19.5 18.0-20.0
Ni (%) 8.0–10.5 <=0.50
P (%) ≤0.045 <=0.040
S (%) ≤0.030 <=0.030
Cb (%) Not specified 0.10-0.60
N (%) Not specified <=0.030
Ti (%) Not specified 0.07-0.30
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property EN 10088-1 1.4301 ASTM A959 .-
Tensile Strength ≥520 MPa Not specified
Yield Strength ≥210 MPa Not specified
Elongation ≥45% Not specified
Hardness ≤215 HB Not specified
Typical Applications
EN 10088-1 1.4301
Food equipment, chemical vessels, architectural, kitchenware
ASTM A959 .-
Wrought stainless steel products; recommended composition limits for adoption by product standards (clause 1.1)
Key Differences
Can EN 10088-1 1.4301 Be Substituted With ASTM A959 .-?
EN 10088-1 1.4301 and ASTM A959 .- share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
Forms & Sizes Available on M-EX
EN 10088-1 1.4301
Sheet → (3 listings)
Thickness: 6–6 mm (0.24–0.24 in)
Width: 1250–1250 mm (49.21–49.21 in)
Length: 2500–3300 mm (98.43–129.92 in)
ASTM A959 .-
No active listings currently.
On M-EX Right Now
EN 10088-1 1.4301
3 active listings and RFQs →
ASTM A959 .-
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10088-1 1.4301 and ASTM A959 .-?
ASTM A959 .- specifies Cb, N, Ti which are not specified for EN 10088-1 1.4301.
Can EN 10088-1 1.4301 be substituted with ASTM A959 .-?
EN 10088-1 1.4301 and ASTM A959 .- share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.