EN 10088-1 1.4301 vs EN 10088-1 X3CrNiCu18-9-4

Close Alternative — 74.9% match based on chemical composition and mechanical property overlap.

EN 10088-1 1.4301 (EN 10088-1:2014) and EN 10088-1 X3CrNiCu18-9-4 (EN 10088-1:2023) are both steel grades. Both fall under the Stainless Steel category. EN 10088-1 1.4301 is defined under European Standard (EN), originating from Europe, while EN 10088-1 X3CrNiCu18-9-4 is defined under European Standard (EN), originating from Europe.

As per chemical composition, EN 10088-1 1.4301 vs EN 10088-1 X3CrNiCu18-9-4 is a 74.9% match. Mechanical property data is not available for both grades, so this factor could not be scored. Combined, this makes them a close alternative overall at 74.9%.

Frequently Compared With EN 10088-1 1.4301:
EN 10088-1 1.4401 EN 10088-1 1.4845 GOST 5632 06Kh23N28 GB/T 3280 06Cr19Ni10 GOST 5632 08X18H10 GOST 5632 12Kh13 EN 10088-1 1.4006 ASTM A959 .- IS 1570 (Part 7) 12Cr13H IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12MoVH ASTM A959 202
Match Breakdown
CHEMISTRY MATCH
74.9%
MECHANICAL MATCH
No shared data
OVERALL
74.9%
Specifications
Property EN 10088-1 1.4301 EN 10088-1 X3CrNiCu18-9-4
Standard EN 10088-1:2014 EN 10088-1:2023
Category Stainless Steel Stainless Steel
C (%) ≤0.07 <=0.04
Si (%) ≤1.00 <=1.00
Mn (%) ≤2.00 <=2.00
Cr (%) 17.5–19.5 17.0-19.0
Ni (%) 8.0–10.5 8.5-10.5
P (%) ≤0.045 <=0.045
S (%) ≤0.030 <=0.015
N (%) Not specified <=0.10
Cu (%) Not specified 3.00-4.0
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property EN 10088-1 1.4301 EN 10088-1 X3CrNiCu18-9-4
Tensile Strength ≥520 MPa Not specified
Yield Strength ≥210 MPa Not specified
Elongation ≥45% Not specified
Hardness ≤215 HB Not specified
Typical Applications
EN 10088-1 1.4301
Food equipment, chemical vessels, architectural, kitchenware
EN 10088-1 X3CrNiCu18-9-4
Not documented
Key Differences
Can EN 10088-1 1.4301 Be Substituted With EN 10088-1 X3CrNiCu18-9-4?
EN 10088-1 1.4301 and EN 10088-1 X3CrNiCu18-9-4 are a close alternative rather than a direct substitute. Some properties overlap well, but check the specific chemistry and mechanical rows above against your application's requirements before treating them as interchangeable.
Forms & Sizes Available on M-EX
EN 10088-1 1.4301
Sheet → (3 listings)
Thickness: 6–6 mm (0.24–0.24 in)
Width: 1250–1250 mm (49.21–49.21 in)
Length: 2500–3300 mm (98.43–129.92 in)
EN 10088-1 X3CrNiCu18-9-4
No active listings currently.
On M-EX Right Now
EN 10088-1 1.4301
3 active listings and RFQs →
EN 10088-1 X3CrNiCu18-9-4
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10088-1 1.4301 and EN 10088-1 X3CrNiCu18-9-4?
EN 10088-1 X3CrNiCu18-9-4 specifies N, Cu which are not specified for EN 10088-1 1.4301.
Can EN 10088-1 1.4301 be substituted with EN 10088-1 X3CrNiCu18-9-4?
EN 10088-1 1.4301 and EN 10088-1 X3CrNiCu18-9-4 are a close alternative rather than a direct substitute. Some properties overlap well, but check the specific chemistry and mechanical rows above against your application's requirements before treating them as interchangeable.