EN 10088-1 1.4845 vs ASTM A240/A240M S34751

Related Material — 69.5% match based on chemical composition and mechanical property overlap.

EN 10088-1 1.4845 (EN 10088-1:2014) and ASTM A240/A240M S34751 (ASTM A240/A240M:2025) are both steel grades. Both fall under the Stainless Steel category. EN 10088-1 1.4845 is typically used for furnace parts, heat exchangers, kiln components, while ASTM A240/A240M S34751 is commonly used for pressure vessels and general applications (plate, sheet and strip). EN 10088-1 1.4845 is defined under European Standard (EN), originating from Europe, while ASTM A240/A240M S34751 is defined under ASTM International, originating from United States.

As per chemical composition, EN 10088-1 1.4845 vs ASTM A240/A240M S34751 is a 54.3% match. As per mechanical properties, the match is 100%. Combined, this makes them a related material overall at 69.5%.

Frequently Compared With EN 10088-1 1.4845:
EN 10088-1 1.4401 EN 10088-1 1.4301 GOST 5632 06Kh23N28 GB/T 3280 06Cr19Ni10 GOST 5632 08X18H10 EN 10088-1 1.4006 GOST 5632 12Kh13 ASTM A959 202 ASTM A959 16-8-2H IS 1570 (Part 7) 12Cr13H ASTM A959 301 ASTM A959 201
Match Breakdown
CHEMISTRY MATCH
54.3%
MECHANICAL MATCH
100%
OVERALL
69.5%
Specifications
Property EN 10088-1 1.4845 ASTM A240/A240M S34751
Standard EN 10088-1:2014 ASTM A240/A240M:2025
Category Stainless Steel Stainless Steel
C (%) ≤0.10 0.005-0.020
Si (%) ≤1.50 <=1.00
Mn (%) ≤2.00 <=2.00
Cr (%) 24.0–26.0 17.0-19.0
Ni (%) 19.0–22.0 9.0-13.0
P (%) Not specified <=0.045
S (%) Not specified <=0.030
N (%) Not specified 0.06-0.10
Nb (%) Not specified 0.20-0.50
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property EN 10088-1 1.4845 ASTM A240/A240M S34751
Tensile Strength ≥515 MPa >=515 MPa
Yield Strength ≥205 MPa >=205 MPa
Elongation ≥40% >=40%
Max Service Temp 1100°C continuous Not specified
Hardness Not specified <=201 HB
Condition Not specified Plate, sheet and strip; yield by 0.2 percent offset
Typical Applications
EN 10088-1 1.4845
Furnace parts, heat exchangers, kiln components
ASTM A240/A240M S34751
Pressure vessels and general applications (plate, sheet and strip)
Key Differences
Can EN 10088-1 1.4845 Be Substituted With ASTM A240/A240M S34751?
EN 10088-1 1.4845 and ASTM A240/A240M S34751 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
Forms & Sizes Available on M-EX
EN 10088-1 1.4845
Sheet → (3 listings)
Thickness: 6–6 mm (0.24–0.24 in)
Width: 1250–1250 mm (49.21–49.21 in)
Length: 2700–3200 mm (106.3–125.98 in)
ASTM A240/A240M S34751
No active listings currently.
On M-EX Right Now
EN 10088-1 1.4845
3 active listings and RFQs →
ASTM A240/A240M S34751
0 active listings and RFQs →
Frequently Asked Questions
What is the difference between EN 10088-1 1.4845 and ASTM A240/A240M S34751?
ASTM A240/A240M S34751 specifies P, S, N, Nb which are not specified for EN 10088-1 1.4845.
Can EN 10088-1 1.4845 be substituted with ASTM A240/A240M S34751?
EN 10088-1 1.4845 and ASTM A240/A240M S34751 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.