GB/T 3280 06Cr19Ni10 vs GOST 5632 12Kh13

Minimal Match — 35% match based on chemical composition and mechanical property overlap.

GB/T 3280 06Cr19Ni10 (GB/T 3280-2015) and GOST 5632 12Kh13 (GOST 5632-2014) are both steel grades. Both fall under the Stainless Steel category. GB/T 3280 06Cr19Ni10 is typically used for used for kitchen equipment, food processing machinery, chemical tanks, piping, architectural panels, and fasteners., while GOST 5632 12Kh13 is commonly used for turbine blades, pump shafts, fasteners, cutlery. GB/T 3280 06Cr19Ni10 is defined under Guobiao Standards (GB/T) (China).

As per chemical composition, GB/T 3280 06Cr19Ni10 vs GOST 5632 12Kh13 is a 62.9% match. As per mechanical properties, the match is 0%. Combined, this makes them a minimal match overall at 35%.

Frequently Compared With GB/T 3280 06Cr19Ni10:
EN 10088-1 1.4845 EN 10088-1 1.4006 EN 10088-1 1.4301 EN 10088-1 1.4401 ASTM A959 .- ASTM A959 16-8-2H IS 1570 (Part 7) 11Cr17Ni13W3TiH IS 1570 (Part 7) 12Cr12Ni2Mo IS 1570 (Part 7) 12Cr13H IS 1570 (Part 7) 12Cr12MoH ASTM A959 202 IS 1570 (Part 7) 12Cr12MoVH
Match Breakdown
CHEMISTRY MATCH
62.9%
MECHANICAL MATCH
0%
OVERALL
35%
Specifications
Property GB/T 3280 06Cr19Ni10 GOST 5632 12Kh13
Standard GB/T 3280-2015 GOST 5632-2014
Category Stainless Steel Stainless Steel
C (%) 0.08 max 0.09–0.15
Si (%) 1.00 max ≤0.80
Mn (%) 2.00 max ≤0.80
Cr (%) 18.00-20.00 12.0–14.0
Ni (%) 8.00-11.00 ≤0.60
P (%) 0.045 max Not specified
S (%) 0.030 max Not specified
Matched by chemical composition and mechanical properties, not a formal equivalence claim. Always verify against the applicable standard before substitution.
Mechanical Properties
Property GB/T 3280 06Cr19Ni10 GOST 5632 12Kh13
Tensile Strength 520-720 MPa ≥540 MPa (annealed)
Yield Strength 205-310 MPa Not specified
Elongation 40-60% Not specified
Hardness 187 HB max Not specified
Hardness HRC Not specified 36–45 (hardened)
Typical Applications
GB/T 3280 06Cr19Ni10
Used for kitchen equipment, food processing machinery, chemical tanks, piping, architectural panels, and fasteners.
GOST 5632 12Kh13
Turbine blades, pump shafts, fasteners, cutlery
Key Differences
Can GB/T 3280 06Cr19Ni10 Be Substituted With GOST 5632 12Kh13?
GB/T 3280 06Cr19Ni10 and GOST 5632 12Kh13 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.
Forms & Sizes Available on M-EX
GB/T 3280 06Cr19Ni10
Sheet → (2 listings)
Thickness: 6–6 mm (0.24–0.24 in)
Width: 1250–1250 mm (49.21–49.21 in)
Length: 2900–3300 mm (114.17–129.92 in)
GOST 5632 12Kh13
Sheet → (2 listings)
Thickness: 6–6 mm (0.24–0.24 in)
Width: 1250–1250 mm (49.21–49.21 in)
Length: 2700–3400 mm (106.3–133.86 in)
On M-EX Right Now
GB/T 3280 06Cr19Ni10
2 active listings and RFQs →
GOST 5632 12Kh13
2 active listings and RFQs →
Frequently Asked Questions
What is the difference between GB/T 3280 06Cr19Ni10 and GOST 5632 12Kh13?
GB/T 3280 06Cr19Ni10 specifies P, S which are not specified for GOST 5632 12Kh13.
Can GB/T 3280 06Cr19Ni10 be substituted with GOST 5632 12Kh13?
GB/T 3280 06Cr19Ni10 and GOST 5632 12Kh13 share some compositional similarity but differ enough that substitution should not be assumed. Review the differences above carefully, and consult the applicable standard or a metallurgist before using one in place of the other.